The influence of nonmetallic inclusions on the fracture properties of A588 Grade A steel plate is investigated by evaluating one plate produced by conventional steel-making practices and another using calcium treatment.
The two plates had differing inclusion structures and their characterization included: tensile, Charpy V-notch, dynamic tear, and J-integral testing; JIc, tearing modulus, and J-Δa and J-T curve determinations on the upper shelf; and fatigue crack propagation and near-threshold fatigue evaluations.

Testing of up to six specimen orientations was used, depending on the testing method. Of all the test methods used in this investigation the JIc and J-T curve determinations were found to be the most sensitive to changes in inclusion structure in all testing orientations. The fatigue crack growth rate of the calcium-treated steel was primarily improved in the through-thickness (SL) orientation at higher ΔK levels. Testing at higher load ratios accentuated these differences.
Oxide and roughness-induced crack closure had a significant effect on the near-threshold fatigue behavior of the conventional steel as a result of the inclusion-induced roughness on the fracture surface. Fractography and crack closure measurements were used to explain this behavior.
What is the difference between Grade A and Grade B A588?
Astm a588 gr a sheet material has a slightly different chemical composition than grade b. The latter has higher copper and chromium levels. Due to the compositional difference, grade b shows more resistance to corrosion than gr a.
What is the difference between A572 and A588?
A572 is primarily used for structural applications requiring high strength, while A588 is specifically designed for outdoor structures subject to atmospheric corrosion. Weathering Properties: A588 develops a protective patina over time when exposed to the environment, enhancing its resistance to atmospheric corrosion.
Can you weld A588 steel?
Typical tensile strength of based metal (weathering steel) is 68-78 KSI. We advise only welding A606-4 or A588 together. Welding A606-4 or A588 to other metals can lead to a dissimilar metal reaction.