What Is ASTM A423 Grade 1 Steel Pipe?
ASTM A423 Grade 1 straight seam steel pipe is a low-alloy steel grade containing controlled amounts of copper, chromium, and nickel. Its chemical composition includes 0.20–0.60% copper, 0.24–1.31% chromium, and 0.20–0.70% nickel. These alloying elements contribute to its resistance to atmospheric and certain industrial corrosion environments.

Unlike ordinary carbon steel tubes, A423 Grade 1 straight seam steel pipe incorporates a defined alloying system to improve corrosion resistance. The material has a minimum tensile strength of 415 MPa, a minimum yield strength of 255 MPa, and a minimum elongation of 25%.
The material is suitable for industrial tubing applications where specified mechanical strength and corrosion resistance are required.
ASTM A423 Gr1 Straight Seam Welded Pipe Manufacturer and Supplier
At Gnee, we supply ASTM A423 Gr1 straight seam welded steel pipe manufactured through the electric-resistance welding (ERW) process. During production, steel strips or coils are prepared, slit to the required width, and gradually formed into a cylindrical shape through forming rolls. The longitudinal edges are then joined by electric resistance welding to create a continuous straight seam.
After welding, the pipe undergoes the required heat treatment and subsequent sizing, straightening, and finishing operations. The weld seam and parent metal are inspected to verify dimensional accuracy and product quality.
For ASTM A423 Grade 1, the standard requires appropriate heat treatment to meet the specified requirements. The final heat treatment condition and manufacturing details are controlled according to the applicable ASTM specification and purchase order.
Our ASTM A423 Grade 1 straight seam steel pipes are supplied with the following mechanical properties:
- Minimum tensile strength: 415 MPa
- Minimum yield strength: 255 MPa
- Minimum elongation: 25%
We can provide straight-length pipes with customized outside diameters, wall thicknesses, and cutting lengths according to project drawings. Available finishing options include black surface, protective coating, shot blasting, and pickling, subject to order requirements.
For customers requiring large straight seam welded pipe, we can evaluate non-standard dimensions and production feasibility according to the required diameter, wall thickness, length, and applicable technical specifications.
ASTM A423 Gr1 Straight Seam Welded Pipe Specification
| Parameter | Specification |
|---|---|
| Standard | ASTM A423/A423M |
| Grade | ASTM A423 Grade 1 |
| Product Type | Straight Seam Welded Steel Pipe |
| Welding Process | Electric Resistance Welding (ERW) |
| Material | Low-Alloy Steel |
| Outside Diameter | 12.7–127 mm (commonly supplied range) |
| Minimum Wall Thickness | 0.9–12.7 mm |
| Length | Customized / 6 m / 12 m |
| Heat Treatment | Normalized or other specified heat treatment |
| Surface Finish | Black / Pickled / Shot Blasted / Coated |
| Pipe Ends | Plain End / Beveled End |
| Inspection | Chemical Analysis / Tensile Test / Flattening Test / Hydrostatic Test or Electric Test |
| Certification | Mill Test Certificate (MTC) EN 10204 3.1 |
Chemical Composition of ASTM A423 Grade 1 Straight Seam Steel Pipe
The chemical composition of ASTM A423 Grade 1 is controlled to ensure that the steel meets the requirements for low-alloy tubing. Copper, chromium, and nickel are the primary alloying elements associated with its corrosion-resistant characteristics.
| Element | Symbol | Composition (%) |
|---|---|---|
| Carbon | C | ≤0.15 |
| Manganese | Mn | ≤0.55 |
| Phosphorus | P | 0.06–0.16 |
| Sulfur | S | ≤0.060 |
| Silicon | Si | ≥0.10 |
| Copper | Cu | 0.20–0.60 |
| Chromium | Cr | 0.24–1.31 |
| Nickel | Ni | 0.20–0.70 |
Mechanical Properties of ASTM A423 Gr1 Straight Seam Welded Steel Pipe
ASTM A423 Grade 1 specifies minimum tensile strength, yield strength, and elongation requirements. These properties are used to evaluate the material's strength and deformation capacity under tensile loading.
| Mechanical Property | Requirement |
|---|---|
| Tensile Strength | ≥415 MPa |
| Yield Strength | ≥255 MPa |
| Elongation in 50 mm | ≥25% |
ASTM A423 Gr1 Straight Seam Welded Pipe Manufacturing Process
The production of ASTM A423 Grade 1 straight seam welded pipe involves several controlled manufacturing stages.
1. Raw Material Inspection
Steel coils are inspected for chemical composition, thickness, width, and surface quality before entering the production line.
2. Strip Slitting
The steel coil is slit into strips according to the required pipe diameter and wall thickness.
3. Forming
The strips pass through a series of forming rolls to create a cylindrical pipe shape with longitudinal edges aligned for welding.
4. ERW Welding
Electric resistance welding joins the longitudinal edges through electrical resistance heating and pressure, forming a continuous straight weld seam.
5. Heat Treatment
The pipe receives the heat treatment required to comply with ASTM A423/A423M and the agreed delivery condition.
6. Sizing and Straightening
Sizing rolls control the outside diameter and roundness, while straightening equipment corrects longitudinal deformation.
7. Cutting and Surface Finishing
The pipe is cut to the specified length. Surface finishing, including pickling, shot blasting, or protective coating, can be arranged according to customer requirements.




Why Choose Pickling Straight Seam Steel Pipe?
Pickling is a surface treatment process used to remove oxide scale, rust, and other surface contaminants from steel pipes through chemical treatment.
For ASTM A423 Grade 1 straight seam welded steel pipe, pickling can be selected when a cleaner metallic surface is required before subsequent processing, inspection, coating, or installation.
The main benefits of pickling include:
Oxide Scale Removal: Removes iron oxide scale generated during hot processing and heat treatment.
Surface Cleaning: Reduces surface contamination before coating or further fabrication.
Improved Surface Inspection: Makes surface defects easier to identify during visual examination.
Preparation for Coating: Provides a cleaned surface for subsequent protective coating processes.


ASTM A423 Grade 1 Straight Seam Welded Pipe Applications
ASTM A423 Grade 1 is specified for low-alloy tubing used in pressure-containing components and applications where corrosion resistance is important. Its established mechanical properties and alloy composition make it suitable for several industrial equipment applications.
1. Power Generation Industry
Used in economizers and related boiler tubing systems where the pipe must meet specified pressure and temperature conditions.
2. Petrochemical Industry
Applied in heat-transfer systems, and industrial piping where material selection is based on the operating medium and corrosion conditions.
3. Chemical Processing Industry
Used in industrial tubing systems and equipment components requiring specified mechanical properties and resistance to certain corrosive environments.
4. Industrial Heat Exchange Systems
Used in heat-transfer equipment where low-alloy steel tubing is selected according to operating temperature, pressure, and fluid characteristics.




ASTM A423 Gr1 Straight Seam Welded Pipe Testing & Inspection
Quality inspection is an essential part of ASTM A423 Grade 1 straight seam welded pipe production. Testing is performed according to the applicable requirements of ASTM A423/A423M and its referenced general requirements.
Chemical Analysis: Verifies the chemical composition of the steel against the specified Grade 1 limits.
Tensile Test: Measures tensile strength, yield strength, and elongation.
Flattening Test: Evaluates the pipe's ability to withstand flattening deformation without unacceptable cracking or defects.
Flaring Test: Evaluates the ductility of the pipe during expansion.
Flange Test: Checks the ability of the pipe end to withstand flanging when applicable.
Hardness Test: Measures material hardness according to the applicable testing requirements.
Hydrostatic Test or Electric Test: Verifies the integrity of the pipe according to the specified test requirements and applicable standard provisions.
Visual and Dimensional Inspection: Checks outside diameter, wall thickness, length, straightness, surface condition, and weld quality.




Additional ultrasonic testing (UT), radiographic testing (RT), and third-party inspection can be arranged when specified in the purchase order.
ASTM A423 Grade 1 Straight Seam Welded Pipe Packaging & Certification
All finished pipes are marked and packed according to the agreed order requirements to maintain product identification and prevent transportation damage.
Marking: Manufacturer's name, ASTM A423/A423M, Grade 1, pipe dimensions, heat number, and other agreed identification details.
Packaging: Pipes can be supplied in bundles with steel or plastic strapping. Protective end caps, moisture-resistant wrapping, and seaworthy wooden packaging are available according to transportation requirements.
Certification: Mill Test Certificate (MTC) with chemical composition and mechanical test results. EN 10204 3.1 certification can be provided when agreed in the order.


ASTM A423 Gr1 Straight Seam Welded Pipe Supplier
Gnee supplies ASTM A423 Grade 1 straight seam welded steel pipes for industrial projects, heat-transfer equipment, and pressure-containing applications.
We support customized pipe dimensions, cutting lengths, pickling, surface finishing, quality inspection, and export packaging. Our sales and technical teams can review your specifications and provide product recommendations based on your project requirements.
To receive a quotation, please provide:
Material Grade: ASTM A423 Grade 1
Outside Diameter (OD): Required diameter in mm or inches
Wall Thickness (WT): Required wall thickness in mm
Length: Fixed length or random length
Quantity: Pieces, meters, or metric tons
Surface Treatment: Black / Pickled / Coated
Inspection Requirements: Standard inspection or additional third-party testing
Destination Port: Country and port of delivery
Contact Gnee today for ASTM A423 Gr1 straight seam welded pipe pricing, technical specifications, and customized supply solutions.