ASTM A423 Grade 1 ERW Corten Steel Tubes are electric resistance welded low-alloy steel tubes designed for pressure-containing components, economizers, and industrial equipment requiring controlled mechanical properties and corrosion resistance.
Manufactured in accordance with ASTM A423/A423M, these ERW steel tubes contain 0.20–0.60% copper, 0.24–1.31% chromium, and 0.20–0.70% nickel, together with controlled carbon, manganese, phosphorus, sulfur, and silicon contents. Their alloy composition provides atmospheric corrosion resistance under suitable exposure conditions.
As an experienced steel supplier, GNEE provides ASTM A423 Gr.1 ERW steel pipes and tubes with customized outside diameters, wall thicknesses, and lengths according to project requirements.



Available product options include ERW welded round steel tubes, cut-to-length tubes, and other agreed configurations. Each order can be supplied with chemical composition reports, mechanical test results, dimensional inspection records, and Mill Test Certificates (MTCs).
ASTM A423 Grade 1 ERW Steel Pipe Scope & Specifications
ASTM A423/A423M covers minimum-wall-thickness electric-resistance welded low-alloy steel tubes for pressure-containing parts, including economizers, and other applications where corrosion resistance is important. Grade 1 is one of the three grades specified in this standard.
The commonly furnished size range is 21-76 mm in outside diameter, with minimum wall thicknesses of 1.5-4.0 mm.
Other dimensions may be supplied when they satisfy the applicable standard requirements and are agreed upon by the purchaser and manufacturer.
| Parameter | ASTM A423 Grade 1 Specification |
|---|---|
| Standard | ASTM A423/A423M; ASME SA423 when specified |
| Grade | Grade 1 |
| Manufacturing Process | ERW (Electric Resistance Welding) |
| Outside Diameter | 21-76 mm, commonly furnished |
| Wall Thickness | 1.5-4.0 mm, minimum wall |
| Length | - |
ASTM A423 Grade 1 ERW Tubes Chemical Composition (wt.%)
The chemical composition of ASTM A423 Grade 1 determines its low-alloy characteristics and contributes to its atmospheric corrosion resistance.
| Symbol | ASTM A423 Grade 1 (wt.%) |
|---|---|
| C | 0.15 max. |
| Mn | 0.55 max. |
| P | 0.06–0.16 |
| S | 0.060 max. |
| Si | 0.10 min. |
| Cu | 0.20–0.60 |
| Cr | 0.24–1.31 |
| Ni | 0.20–0.70 |
ASTM A423 Grade 1 ERW Steel Tubes Mechanical Properties
ASTM A423 Grade 1 ERW steel tubes must meet the tensile requirements specified by ASTM A423/A423M.
| Mechanical Property | ASTM A423 Grade 1 Requirement |
|---|---|
| Tensile Strength | 60 ksi (415 MPa) min. |
| Yield Strength | 37 ksi (255 MPa) min. |
| Elongation in 2 in. (50 mm) | 25% min. |
ASTM A423 Grade 1 ERW Steel Tubes Testing & Inspection
Quality inspection is necessary to verify the chemical composition, mechanical properties, weld integrity, and dimensional accuracy of ASTM A423 Grade 1 ERW steel tubes. Testing requirements are determined by ASTM A423/A423M, applicable general requirements, and the purchase order.
| Test |
|---|
| Chemical Analysis |
| Tensile Test |
| Flattening Test |
| Flaring Test |
| Flange Test |
| Hardness Test |
| Hydrostatic Test |
| Nondestructive Electric Test |




ASTM A423 Grade 1 ERW Corten Steel Tubes Applications
ASTM A423 Grade 1 ERW Corten Steel Tubes are used in industrial equipment where low-alloy steel tubing, pressure resistance, and corrosion resistance are required. Their copper- and chromium-containing composition makes them suitable for selected atmospheric and industrial service conditions.
| Industry |
|---|
| Power Generation |
| Boiler Manufacturing |
| Chemical Processing |
| Sugar Industry |
| Petrochemical Industry |
| Waste Heat Recovery |
A. ERW Boiler Tubes and Economizer Tubes
ASTM A423 Grade 1 ERW Boiler Tubes can be specified for applicable economizer and other pressure-containing tube components. In an economizer, water flows through tube circuits while hot flue gas transfers heat to the tube walls. The material grade, operating temperature, pressure, corrosion conditions, and tube dimensions must all be checked against the equipment design requirements.
B. ERW Heat Exchanger Steel Tubes
In industrial heat exchangers, ERW steel tubes serve as heat-transfer components that separate different fluid streams. The specified outside diameter, minimum wall thickness, tube length, and mechanical properties must match the heat exchanger design and operating conditions.



Why Choose GNEE as Your ASTM A423 Grade 1 ERW Steel Pipe Supplier?
Selecting an ERW steel pipe supplier involves more than comparing the unit price. Material traceability, manufacturing capabilities, inspection records, dimensional control, and delivery arrangements all affect the final procurement result.
GNEE provides steel pipe supply services for industrial equipment manufacturers, engineering contractors, and international distributors. Our supply services include:
- ASTM Standard Compliance: Supply according to ASTM A423/A423M and agreed purchase specifications.
- Customized Dimensions: Confirm outside diameter, wall thickness, and cut length according to project drawings.
- Quality Documentation: Provide MTCs, chemical analysis, mechanical test reports, and inspection records.
- Order Inspection: Arrange dimensional inspection and agreed additional testing before shipment.
- Export Packaging: Arrange protective packaging and shipping marks according to transportation requirements.
- International Delivery: Coordinate production schedules, export documentation, and shipment arrangements.
Request a Quote for ASTM A423 Grade 1 ERW Corten Steel Tubes
Looking for a reliable ERW Corten Steel Tubes supplier for your boiler, economizer, air preheater, or industrial heat-transfer project?
GNEE can provide ASTM A423 Gr.1 ERW steel tubes according to your required dimensions, quantities, and inspection specifications. Send us your technical drawings or inquiry details to receive a product confirmation and quotation.
To receive an accurate quotation, please provide:
- Material Grade: ASTM A423 Gr.1 / ASME SA423 Gr.1
- Manufacturing Process: ERW
- Outside Diameter (OD): Required diameter in mm or inches
- Wall Thickness (WT): Required thickness in mm or inches
- Length: Random Length or Cut-to-Length
- Quantity: Required quantity in tons or pieces
- Inspection Requirements: MTC, Hydrostatic Test, NDT, or Third-Party Inspection
- Destination Port: Delivery destination
Contact GNEE Today for Your ASTM A423 Grade 1 ERW Steel Pipe Quotation.