What Is ASTM A423/A423M Standard?
ASTM A423/A423M is a standard specification covering seamless and electric-resistance welded low-alloy steel tubes for pressure-containing components, including boiler economizers and other applications where atmospheric corrosion resistance is important.
It covers three material grades: ASTM A423 Grade 1, Grade 2, and Grade 3. The standard specifies chemical composition, tensile properties, manufacturing conditions, heat treatment, and inspection requirements to ensure the tubes meet the requirements of their intended service conditions.
What Is Corten Steel ASTM A423 Gr.1 Heat Exchanger Tubes?
Corten Steel ASTM A423 Gr.1 heat exchanger tubes are low-alloy steel tubes containing controlled amounts of copper (Cu), chromium (Cr), and nickel (Ni). These alloying elements contribute to atmospheric corrosion resistance and help reduce the corrosion rate under suitable environmental conditions.
ASTM A423 Grade 1 heat exchanger tubes are manufactured through seamless or electric-resistance welded processes. Electric-resistance welded (ERW) tubes are produced by forming steel strip into a tubular shape and joining the longitudinal edges through electrical resistance heating and pressure.
With a minimum tensile strength of 415 MPa and a minimum yield strength of 255 MPa, A423 Gr.1 steel tubes are used in heat exchangers, boiler economizers, air preheaters, steam-generating equipment, and industrial heat recovery systems.



ASTM A423 Gr.1 Heat Exchanger Tubes Manufacturing Process
ASTM A423 Grade 1 heat exchanger tubes are available in seamless and electric-resistance welded types. The manufacturing route depends on the required tube dimensions, production quantity, and project specifications.
For welded A423 Gr.1 heat exchanger tubes, the typical manufacturing process includes:
- Raw Material Inspection: Verify the chemical composition, material grade, surface condition, and heat number of the steel strip or coil.
- Strip Slitting: Cut the steel coil into strips according to the required tube circumference and dimensional requirements.
- Roll Forming: Pass the steel strip through forming rolls to gradually create an open tubular section.
- Electric Resistance Welding: Join the longitudinal edges through electrical resistance heating and mechanical pressure.
- Weld Seam Inspection: Examine the longitudinal weld seam using suitable nondestructive testing methods.
- Sizing and Straightening: Adjust the outside diameter, wall thickness profile, and straightness to meet the specified dimensions.
- Heat Treatment: Apply the required normalizing or other heat treatment to meet ASTM A423 requirements.
- Cutting and Final Inspection: Cut the tubes to the ordered length and inspect their dimensions, surface condition, and mechanical properties.




ASTM A423 Gr.1 Heat Exchanger Tubes Specifications & Standards
| Parameter | Technical Specification |
|---|---|
| Product Name | ASTM A423 Gr.1 Heat Exchanger Tubes |
| Material Grade | ASTM A423 Grade 1 |
| Governing Standard | ASTM A423/A423M |
| Tube Type | Electric-Resistance Welded |
| Manufacturing Process | Hot Finished / Cold Finished |
| Outside Diameter | 21-76 mm (standard usual supply range) |
| Wall Thickness | 1.5-4.0 mm (minimum-wall specification range) |
| Length | 3,000–12,000 mm, customizable by agreement |
| Heat Treatment | Normalized or as required by ASTM A423 |
| End Finish | Plain End / Beveled End |
| Certification | EN 10204 3.1 / 3.2, subject to order requirements |
Note: ASTM A423 commonly covers outside diameters of 21-76 mm and minimum wall thicknesses of 1.5-4.0 mm.
ASTM A423 Grade 1 Heat Exchanger Tubes Chemical Composition (wt.%)
The chemical composition of ASTM A423 Grade 1 includes copper, chromium, and nickel as the principal alloying elements contributing to its atmospheric corrosion resistance.
| Element | ASTM A423 Grade 1 (wt.%) |
|---|---|
| Carbon (C) | ≤0.15 |
| Manganese (Mn) | ≤0.55 |
| Phosphorus (P) | 0.06–0.16 |
| Sulfur (S) | ≤0.060 |
| Silicon (Si) | ≥0.10 |
| Copper (Cu) | 0.20–0.60 |
| Chromium (Cr) | 0.24–1.31 |
| Nickel (Ni) | 0.20–0.70 |
ASTM A423 Gr.1 Heat Exchanger Tubes Mechanical Properties
ASTM A423 Grade 1 heat exchanger tubes are specified with a minimum tensile strength of 415 MPa and a minimum yield strength of 255 MPa. The minimum elongation requirement is 25%.
| Mechanical Property | ASTM A423 Grade 1 |
|---|---|
| Tensile Strength | ≥415 MPa |
| Yield Strength | ≥255 MPa |
| Elongation | ≥25% |
| Hardness | As specified by applicable ASTM requirements |
ASTM A423 Gr.1 Heat Exchanger Tube Size and Dimensional Requirements
ASTM A423 Grade 1 heat exchanger tube size selection depends on the heat exchanger design, operating pressure, heat transfer requirements, and installation conditions. The outside diameter and wall thickness directly influence the internal flow area, pressure-bearing capacity, and heat transfer surface area.
For common industrial applications, the standard supply range is 21-76 mm in outside diameter and 1.5-4.0 mm in minimum wall thickness. Custom A423 Grade 1 heat exchanger tubes can also be produced according to drawings and agreed dimensional requirements.
| Dimension | Standard Supply Range |
|---|---|
| Outside Diameter (OD) | 21-76 mm |
| Wall Thickness (WT) | 1.5-4.0 mm |
| Length | 3–12 m |
| Tube Type | ERW |
| Custom Dimensions | Available upon agreement |
Corrosion Resistance of ASTM A423 Grade 1 Heat Exchanger Tubes
ASTM A423 Grade 1 heat exchanger tubes are manufactured with a copper-chromium-nickel alloy composition designed to improve atmospheric corrosion resistance. According to ASTM A423/A423M, the material contains 0.20–0.60% copper (Cu), 0.24–1.31% chromium (Cr), and 0.20–0.70% nickel (Ni).
Compared with Q235B carbon steel, which has residual element limits of 0.30% maximum for copper, chromium, and nickel under GB/T 700-2006, A423 Grade 1 has specifically controlled alloying ranges for these elements. In particular, its chromium content can reach 1.31%, providing a substantially different alloy composition from conventional Q235B structural steel.
The combined effects of copper, chromium, and nickel contribute to the development of a more protective and adherent corrosion product layer under suitable atmospheric exposure conditions. This helps improve the material's resistance to atmospheric corrosion and makes A423 Gr.1 a suitable material option for heat exchanger components exposed to humid industrial environments and outdoor conditions.
STM A423 Gr.1 Heat Exchanger Tubes Applications
ASTM A423 Grade 1 heat exchanger tubes are used in industrial equipment where low-alloy steel strength and atmospheric corrosion resistance are required. Their common applications include:
| Application |
|---|
| Boiler Economizers |
| Air Preheaters |
| Industrial Heat Exchangers |
| Shell-and-Tube Heat Exchangers |
| Power Generation Equipment |
| Waste Heat Recovery Systems |
| Steam Generating Equipment |



Quality Control and Testing of ASTM A423 Grade 1 Heat Exchanger Tubes
GNEE applies material inspection, dimensional verification, mechanical testing, and applicable nondestructive testing procedures to ASTM A423 Grade 1 heat exchanger tubes.
Inspection requirements are determined according to ASTM A423 and the technical specifications agreed upon in the purchase order.
| Test / Inspection Item |
|---|
| Chemical Composition Analysis |
| Tensile Test |
| Flattening Test |
| Flaring Test |
| Flange Test |
| Reverse Flattening Test |
| Hydrostatic Test |
| Hardness Test |
| Ultrasonic Testing (UT) |
| Dimensional Inspection |
| Visual Inspection |
Each batch can be supplied with a Material Test Certificate (MTC) containing the heat number, chemical composition, mechanical test results, and relevant inspection records. Third-party inspection by SGS, BV, or Intertek can be arranged according to customer requirements.




ASTM A423 Gr.1 Heat Exchanger Tube Manufacturers and Suppliers
GNEE supplies ASTM A423 Grade 1 heat exchanger tubes for industrial heat transfer, boiler economizer, and power generation projects. We provide seamless and electric-resistance welded tube options according to project specifications, including customized outside diameters, wall thicknesses, and lengths. Our supply services include:
- ASTM A423 Grade 1 material supply.
- ERW heat exchanger tubes.
- Customized heat exchanger tube sizes.
- Chemical composition and mechanical property inspection.
- Material Test Certificates (MTC).
- Third-party inspection arrangements.
- Export packaging and international shipment.
Whether you are sourcing A423 Gr.1 welded heat exchanger tubes for a new project or comparing A423 Grade 1 heat exchanger tube prices for bulk procurement, our sales and technical teams can assist with material selection, dimensional confirmation, and quotation preparation.
Request a Quote for ASTM A423 Gr.1 Heat Exchanger Tubes
Looking for reliable ASTM A423 Gr.1 heat exchanger tube manufacturers and suppliers? Contact GNEE for:
- Competitive A423 Gr.1 heat exchanger tube prices.
- Customized OD, wall thickness, and tube length.
- ASTM A423/A423M material compliance.
- Chemical and mechanical test documentation.
- Bulk orders and international delivery.
Send us your required tube size, wall thickness, quantity, and technical specifications today. Our team will provide a product recommendation and quotation based on your project requirements.