A423 Gr.1 corten steel air heater tubes

Nov 20, 2026 Leave a message

What Is the ASTM A423/A423M Standard?

ASTM A423/A423M is the standard specification for seamless and electric-resistance-welded low-alloy steel tubes. It covers minimum-wall-thickness tubes used in pressure-containing components, including boiler economizers and other industrial equipment where corrosion resistance is required.

 

ASTM A423 Grade 1 is a low-alloy steel. Its chemical composition is designed for applications requiring a combination of mechanical strength and resistance to atmospheric corrosion. It is used in boiler equipment, air preheaters, economizers, and industrial heat-exchange systems.

 

What Are A423 Gr.1 Corten Steel Air Heater Tubes?

A423 Gr.1 Corten steel air heater tubes are low-alloy steel tubes manufactured according to ASTM A423/A423M Grade 1 requirements. They are used in air preheaters (APH), boiler heat recovery systems and industrial heat exchangers to transfer thermal energy between hot flue gas and incoming combustion air.

 

These tubes are commonly manufactured using the electric-resistance welding (ERW) process. Steel strips are formed into round tubular sections, and their longitudinal edges are joined through electrical resistance heating and pressure. The welded seam is subsequently processed and inspected according to the applicable manufacturing and quality requirements.

 

The copper content of 0.20–0.60%, chromium content of 0.24–1.31% and nickel content of 0.20–0.70% contribute to the atmospheric corrosion characteristics of ASTM A423 Grade 1. Under suitable atmospheric exposure conditions, these elements participate in the formation of corrosion products that can reduce further atmospheric attack.

A423 Gr.1 Corten Steel Air Heater Tubes
A423 Gr.1 Corten Steel Air Heater Tube
A423 Gr.1  Air Heater Tubes

A423 Grade 1 Air Heater Tube Specifications

Parameter  Specification
Material Grade ASTM A423 Grade 1
Standard  ASTM A423/A423M
Welding Process  Electric Resistance Welding (ERW)
Outside Diameter 21-76 mm
Wall Thickness  1.5-4.0 mm
Tube Length  3–12 m or customized
Surface Condition  Black / Oiled / As Manufactured

 

Chemical Composition of ASTM A423 Grade 1 (wt.%)

The chemical composition of ASTM A423 Grade 1 determines its low-alloy characteristics and atmospheric corrosion performance. Copper, chromium and nickel are the main alloying elements associated with its atmospheric corrosion resistance.

Element ASTM A423 Grade 1 (%)
Carbon (C)  ≤ 0.15
Silicon (Si)  ≥ 0.10
Manganese (Mn)  ≤ 0.55
Phosphorus (P) 0.06–0.16
Sulfur (S) ≤ 0.060
Copper (Cu)  0.20–0.60
Chromium (Cr)  0.24–1.31
Nickel (Ni)  0.20–0.70
Iron (Fe)  -

 

Mechanical Properties of A423 Grade 1 Steel Tubes

ASTM A423 Grade 1 steel tubes are required to meet the specified tensile strength, yield strength and elongation requirements. These mechanical properties are important for tube forming, installation, bending and pressure-containing applications.

Mechanical Property  Requirement 
Tensile Strength ≥ 415 MPa
Yield Strength ≥ 255 MPa
Elongation in 50 mm  ≥ 25%

 

Heat Exchanger Tube Sizes, Lengths and Wall Thickness

When selecting A423 Grade 1 heat exchanger tubes, outside diameter, wall thickness and tube length must be considered together. These dimensions directly affect the tube's internal flow area, heat-transfer surface area, pressure design and installation compatibility.

 

The standard ASTM A423/A423M commonly covers outside diameters from 12.7 mm to 127 mm and minimum wall thicknesses from 0.9 mm to 12.7 mm.

 

Other dimensions may be supplied when they comply with the remaining requirements of the standard and are agreed upon by the purchaser and manufacturer.

 

Heat Exchanger Tube Size Reference

Outside Diameter (mm) Wall Thickness (mm)  Length (m) 
19.05 1.0–3.0 3–12
22.20 1.0–3.5 3–12
25.40 1.0–4.0 3–12
31.75 1.2–4.5 3–12
33.70 1.2–5.0 3–12
38.10 1.5–5.0 3–12
44.45 1.5–5.5 3–12
50.80 1.5–6.0 3–12
57.15 1.5–6.0 3–12
60.30 2.0–6.0 3–12
63.50 2.0–6.5 3–12
76.20 2.0–8.0 3–12
88.90 2.5–9.0 3–12
101.60 3.0–10.0 3–12
114.30 3.0–10.0 3–12
127.00 3.0–12.7 3–12

 

Atmospheric Corrosion Resistance of ASTM A423 Grade 1 Air Preheater Tubes

ASTM A423 Grade 1 contains three important alloying elements that influence atmospheric corrosion behavior:

Alloying Element Content (%) 
Copper (Cu)  0.20–0.60
Chromium (Cr)  0.24–1.31
Nickel (Ni)  0.20–0.70

During atmospheric exposure, the surface of suitable weathering steel can develop a relatively adherent oxide layer. The development and stability of this layer depend on repeated wetting and drying cycles, atmospheric composition and exposure conditions.

 

For air preheater applications, corrosion behavior is also affected by flue gas composition and the possibility of acid condensation. When the metal surface temperature falls below the acid dew point, sulfuric acid condensate may form and cause accelerated corrosion.

 

Therefore, ASTM A423 Grade 1 should be selected according to the actual flue gas environment, temperature distribution and equipment operating conditions. It should not be regarded as immune to acid corrosion or as a replacement for specialized corrosion-resistant materials in every application.

 

Applications of A423 Grade 1 Corten Steel Air Heater Tubes

A423 Grade 1 steel tubes are used in industrial equipment that requires heat transfer and atmospheric corrosion resistance. Their main applications include:

1. Boiler Air Preheaters

Air preheaters recover heat from boiler exhaust gases and transfer it to incoming combustion air. A423 Grade 1 air preheater tubes can be used as heat-transfer elements in tubular air preheater systems.

 

2. Boiler Economizers

Economizers recover heat from flue gases to increase boiler feedwater temperature before water enters the boiler. A423 Grade 1 tubes are suitable for specified economizer applications requiring low-alloy steel tubes.

 

3. Industrial Heat Exchangers

A423 Grade 1 heat exchanger steel tubes can be used in equipment where heat is transferred between two fluids through a tube wall. Tube diameter, wall thickness, length and pressure requirements must be determined according to the equipment design.

 

4. Power Generation Equipment

Power plants use air preheaters, economizers and other heat-recovery equipment to improve thermal efficiency. ASTM A423 Grade 1 tubes can be specified for applicable boiler heat-transfer components.

 

5. Waste Heat Recovery Systems

Industrial furnaces and combustion systems discharge hot exhaust gases. Heat recovery equipment can transfer part of this energy to incoming air or other process fluids.

Corten Steel Air Heater Tubes
ASTM A423 Grade 1 Tubes
A423 Grade 1 heat exchanger tube
ASTM A423 Grade 1 heat exchanger tube

Quality Control and Inspection of ASTM A423 Grade 1 Tubes

Quality inspection is an important part of A423 Grade 1 heat exchanger tube manufacturing. Each inspection item should be performed according to ASTM A423/A423M and the additional requirements stated in the purchase order.

Inspection Item 
Chemical Composition
Tensile Test 
Flattening Test 
Flaring Test
Hydrostatic Test 
Dimensional Inspection
Surface Inspection 
Nondestructive Examination
A423 Grade 1 Heat Exchanger Tubes
A423 Gr.1 Corten Steel Air Heater Tubes
ASTM A423 Grade 1 Air Preheater Tube

Why Choose GNEE as Your A423 Grade 1 Heat Exchanger Tubes Manufacturer?

GNEE supplies ASTM A423 Grade 1 steel tubes for boiler equipment, air preheaters, economizers and industrial heat exchangers.

We provide product specifications and supply arrangements according to project requirements, including:

  • Material Grade: ASTM A423 Grade 1 / ASME SA423 Grade 1.
  • Manufacturing Type: ERW and other available manufacturing types subject to specification.
  • Outside Diameter: 21-76 mm standard reference range.
  • Wall Thickness: 1.5-4.0 mm standard reference range.
  • Tube Lengths: 3–12 m and customized lengths.
  • Quality Documents: Mill Test Certificate (MTC), chemical analysis and mechanical test reports.
  • Inspection: Dimensional inspection, surface inspection and specified mechanical or nondestructive tests.
  • Packaging: Steel-strapped bundles, protective wrapping and customized export packaging.

 

As an A423 Grade 1 heat exchanger tubes manufacturer and supplier, GNEE can assist customers in confirming tube specifications, material requirements, order quantities and delivery arrangements.

 

Request a Quote for A423 Grade 1 Corten Steel Air Heater Tubes

 

Looking for ASTM A423 Grade 1 corten steel air heater tubes for your boiler or heat exchanger project?

 

Contact GNEE to obtain product specifications, available sizes, customized tube lengths and a competitive quotation. To receive an accurate quotation, please provide:

  • Material Grade: ASTM A423 Grade 1 or ASME SA423 Grade 1.
  • Outside Diameter (OD).
  • Wall Thickness (WT).
  • Required Tube Length.
  • Quantity.
  • Manufacturing Type: ERW or Seamless.
  • Required Inspection and Certification.
  • Delivery Destination.
ASTM A423 Grade 1 corten steel air heater tubes
A423 Grade 1 Heat Exchanger Steel Tubes
A423 Grade 1 Air Heater Tubes