1. Q355NHD flower boxes can be anti-corrosion treated (optional, not mandatory)

2. Recommended anti-corrosion treatments for Q355NHD flower boxes (matching application scenarios)
Pre-weathering treatment: Factory-induced controlled oxidation to form a preliminary dense patina; eliminates on-site rust powder shedding, prevents soil/flower pot staining, and shortens the patina maturation period to 1–3 months.
Transparent weathering sealer coating: Brushes/sprays a special water-based transparent sealer for weathering steel; traps loose rust powder in the initial stage, does not block natural patina growth, and maintains the original corten steel texture while preventing water seepage into micro-cracks.
Pickling + passivation: Removes surface oxide scale and impurities; ensures uniform initial oxidation of the flower box surface, avoids localized uneven rusting, and lays a good foundation for subsequent patina formation (suitable for as-rolled Q355NHD plates).

3. Not recommended anti-corrosion treatments for Q355NHD flower boxes
Full painting/epoxy coating (completely covers the steel surface, stops patina formation)
Hot-dip galvanizing/electro-galvanizing (zinc layer conflicts with patina formation, and sacrificial anode effect is unnecessary for weathering steel)
Heavy anti-rust primer (hides the corten steel texture and causes coating bubbling when the steel naturally oxidizes)

4. Key considerations for anti-corrosion treatment of Q355NHD flower boxes
Targeted treatment for key areas: Focus on welding seams, cutting edges and bottom contact surfaces (prone to water accumulation/soil corrosion) for local sealer coating, without full-surface treatment to retain the natural patina aesthetic of the main body.
Post-treatment maintenance: Avoid frequent cleaning with acidic/alkaline detergents after treatment; simply wipe off surface dust with clean water to not damage the preliminary patina or sealer layer.
Harsh environment adaptation: In high-humidity coastal/salt-spray or heavy industrial areas, apply a second thin sealer coating after the patina matures to enhance the corrosion resistance of the flower box without affecting color stability.