EN 10155 S355J0WP corten steel plate for outdoor sculpture

Oct 24, 2025 Leave a message

Products Description

 

S355J0WP is a type of weather-resistant structural steel, also known as atmospheric corrosion-resistant steel. It contains copper, chromium, and nickel as the main alloying elements, with added phosphorus that enhances its self-protective performance.

info-445-445

When exposed to air and moisture, a stable oxide layer (patina) gradually forms on the surface, effectively shielding the inner steel from further corrosion and eliminating the need for painting.

 

Products Specification

 

Gnee Grade :

S355J0WP

Specification:

Thickness 8mm-300mm, Width: 1500-4020mm, Length: 3000-27000mm

Standard:

EN10025-5 Technical delivery conditions for general structural steels

Approval By Third Party

ABS, DNV, GL, CCS, LR , RINA, KR, TUV, CE

Classification:

hot rolled or normalizing structural steels

 

Chemical composition % of the Product analysis of grade S355J0WP

 

C

Si

Mn

Cu

P

S

Cr

N

0.15

0.80

1.10

0.20-0.60

0.05-0.16

0.040

0.25-1.35

0.010

 

Mechanical properties of grade S355J0WP

 

Temperature

-20

-10

0

20

Notch impact test. Min. absorbed energy J

 

 

27

 

 

Nominal thickness (mm)

to 16

16 - 40

40 - 63

63 - 80

80 - 100

100 - 150

ReH - Minimum yield strength (MPa)

355

345

 

 

 

 

 

Nominal thickness (mm)

to 3

 

3 - 100

 

100-150

Rm -Tensile strength (MPa)

510-680

 

470-630

 

 

Nominal thickness (mm)

≥1.5<2

≥2﹤2.5

 

≥2.5<3

 

≥3<40

≥40﹤63

≥6﹤100

≥100﹤150

A - Minimum elongation Lo = 5,65 √ So (%) Longitudinal

 

16

 

17

 

18

 

22

 

 

 

 

 

 

 

 

Products Application

 

S355J0WP is a structural weathering steel renowned for its exceptional atmospheric corrosion resistance, making it an ideal material for outdoor architectural projects and sculptures.

 

Its unique alloy composition-primarily chromium, copper, nickel, and phosphorus-allows it to form a stable rust-like patina when exposed to the atmosphere.

 

This patina serves as a protective layer, shielding the steel from further corrosion and eliminating the need for painting or regular maintenance.

 

Outdoor Architectural Facades

Usage: Cladding, curtain walls, decorative panels, pergolas, canopies, and public building facades.

Advantages:

Forms a rust-colored finish that blends naturally with landscapes.

Low maintenance: no repainting required for decades, reducing long-term operational costs by 30–50% compared to painted steel.

Durable in various climates: effective in humid, coastal, or industrial environments.

 

Outdoor Sculptures

Usage: Public art installations, landscape sculptures, monuments, and decorative urban elements.

 

Advantages:

The natural rust patina provides aesthetic appeal, creating a warm, earthy tone that evolves over time.

 

The steel's mechanical strength (tensile 390–550 MPa, yield ≥245 MPa) allows large-scale sculptures to be fabricated without additional internal support in most cases.

 

Resistant to acid rain and pollution, ensuring long-term stability of exposed sculptures.

 

Contact now to get S355J0WP Quote

 

info-536-393