S355J2W+N is a specialized weathering steel grade with an addition of nickel (N) in its chemical composition. EN 10025 5 s355j2w n plate shows improved weathering properties compared to standard S355J2W.
Thus, it is preferred for outdoor structures that are subjected to harsh environmental conditions.

S355J2W+N plate forms a protective patina on its surface which reduces the need for maintenance and painting.
Weathering steel S355J2W+N plate can be used in bridges, facades, containers, railway vehicles and structural components. Their properties like weathering resistance and high strength enhance their longevity and performance.
S355J2W+N plate specification
| Thickness | Width | Length |
|---|---|---|
| 6 to 200 mm | 1500 to 4050 mm | 3000 to 15000 mm |
| Standard | Make Available | Process |
| EN 10025-5 | Jindal, Uttam | Hot -Rolled (HR) |
S355j2w+n sheet mechanical properties
| Tensile Strength | Yield Strength | Minimum Elongation A (Lo = 5.65 vSo) % |
|---|---|---|
| 510 – 680 MPa | 355 MPa | 20 |
Weathering steel s355j2w+n Plate chemical properties
| P | C | CEV | Mn | Si | Cr | S | Zr | Cu | Ni | Mo |
|---|---|---|---|---|---|---|---|---|---|---|
| 0.03 max. | 0.16 max. | 0.44 max. | 0.50 max. | 0.50 max. | 0.40-0.80 | 0.03 max. | 0.15 max. | 0.25-0.55 | 0.65 max. | 0.03 max. |
EN10025 s355j2w+n steel plate equivalent
| W. Nr. | USA | EN | DIN | JIS | BS | AFNOR |
|---|---|---|---|---|---|---|
| 1.8965 | A588Gr.A A600A A600B A600 |
S355J2G1W Fe510D2KI |
WSt52.3 | SMA570W | WR50C | E36WB4 |
Impact properties of S355J2W+N sheet
| Temperature (°C) | 0°C |
| Notch Impact Energy (J) | ≥ 27 |
Contact now to get s355j2w+n Quote

FAQ
Q: What is the meaning of S355J2W N?
A: S355J2W+N is a specialized weathering steel grade with an addition of nickel (N) in its chemical composition.
Q: What is S355J2 N steel grade?
A: S355J2+N is a non-alloy structural steel that has excellent cold-forming properties. It is tensile strength between 490 and 630 N/mm2. They are produced per the requirements & regulations for the relevant items. Structural steel plates of the S355J2+N EN 10025-2 size range from 101mm to 200mm
Q: What is the equivalent material of S355J2 N?
A: The S355j2+n equivalent material is DIN 17100, St52-3N, JIS G3106, SM490YB, and ASTM A572-50.
Q: S355j2w+n VS S355j2+n
A: S355J2W+N sheets material is a weathering steel grade with enhanced atmospheric corrosion resistance due to the addition of Ni. It is specifically used in outdoor applications that are exposed to harsh weather conditions.
S355J2+N is a non alloy structural steel grade used for general structural purposes. It has lower level of corrosion resistance compared to S355J2W+N sheets.
Q: How much time it take to get s355j2w+n steel plate ?
A: 1.The time taken to obtain the S355J2W+N steel plate can depend on:
2.The order quantity, dimensional specifications and the customization required.
If the plates are in stock, the lead time can be relatively short like a few days to a week. However, if the S355J2W+N structural steel plates need to be manufactured or sourced, the delivery timelines can be stretched.