How does the thickness of ASTM A588 GrB weathering steel affect its mechanical properties?

Feb 13, 2026 Leave a message

As thickness increases, the mechanical properties of ASTM A588 Gr.B decrease gradually due to differences in cooling rate, microstructure homogeneity, and internal stress during hot rolling.
 
Yield Strength
 
Thinner sections cool faster and have a finer, stronger microstructure, so they achieve higher yield strength.
 
As thickness increases, the core cools more slowly, resulting in lower strength.
 

≤ 100 mm: ≥ 345 MPa

100–125 mm: ≥ 315 MPa

125–200 mm: ≥ 290 MPa

info-609-368

Tensile Strength
 
Similar to yield strength, tensile strength also reduces with increasing thickness.
 

≤ 100 mm: ≥ 485 MPa

100–125 mm: ≥ 460 MPa

125–200 mm: ≥ 435 MPa

 
Elongation & Ductility
 
Thicker plates often show slightly lower elongation because of coarser grains and more internal inhomogeneity.
 
However, all grades still meet the minimum elongation requirements for structural use.

info-313-282

Toughness
 
Thicker plates are more prone to centerline segregation and slower transformation, which can reduce low-temperature impact toughness.
 
Thinner plates generally exhibit better and more consistent toughness.
 
Uniformity of Properties
 
Thinner plates have more uniform through-thickness properties.
 

Thicker plates show greater variation between surface and core, leading to lower guaranteed minimum strengths.

info-455-436