In general, the yield strength of ASTM A588 Gr.B weathering steel varies significantly with temperature, following typical behavior for structural carbon–manganese weathering steels.

At low temperatures (below room temperature, down to −40 °C)
As temperature decreases, yield strength increases gradually, while ductility and toughness decrease.
This means the steel becomes stronger but more brittle, so it is more sensitive to impact loading.
However, A588 Gr.B is designed with good low‑temperature toughness, so it remains suitable for many cold‑environment structural applications.
At room temperature to approximately 200 °C
Yield strength remains relatively stable, with only a slight decrease.
Tensile strength also stays close to room‑temperature values.
This range covers nearly all normal outdoor and industrial service conditions, so structural performance is reliable.

From 200 °C to 400 °C
Yield strength drops noticeably as temperature rises.
The steel softens progressively, so its ability to resist deformation under load is reduced.
Prolonged exposure in this range can lead to increased deflection in structural members.
Above 400 °C
Yield strength decreases rapidly and the material loses significant load‑bearing capacity.
Microstructural stability declines, and the steel cannot be relied upon for structural safety.
A588 Gr.B is not intended for high‑temperature service such as boilers or high‑heat equipment.