What is JIS G 3125 SPA-H corten steel plate weather resistant steel sheet

Jan 05, 2026 Leave a message

What Is JIS G 3125 SPA-H Steel Plate?

 

JIS G 3125 SPA-H steel plate is a hot-rolled atmospheric corrosion-resistant steel, commonly known as Corten steel or weathering steel.

 

It is designed to offer significantly better resistance to atmospheric corrosion than ordinary carbon steel, with or without copper additions.

When exposed to outdoor environments, SPA-H steel forms a stable, dense rust-like oxide layer on its surface.

 

JIS G 3125 SPA-H steel plate

This protective patina slows down further corrosion, allowing the steel to be used without painting or with reduced coating systems, thereby lowering long-term maintenance costs.

 

Standard of JIS G 3125 SPA-H Steel Plate

 

JIS G 3125 is a Japanese Industrial Standard covering hot-rolled steel plates, sheets, and strips for superior atmospheric corrosion resistance. SPA-H is one of the main grades specified under this standard.

 

Chemical Composition

 

Grade C ≤ Si Mn ≤ P S ≤ Cu Cr Ni ≤
SPA-H 0.12 0.20–0.75 0.60 0.070–0.150 0.035 0.25–0.55 0.30–1.25 0.65

 

The addition of alloying elements such as Cu, Cr, and Ni enhances the steel's atmospheric corrosion resistance and contributes to its stable protective oxide layer.

 

Mechanical Properties

 

Plate Thickness Yield Strength Tensile Strength Elongation
≤ 6.0 mm ≥ 355 MPa ≥ 490 MPa ≥ 22%
> 6.0 mm ≥ 355 MPa ≥ 490 MPa ≥ 15%

SPA-H steel combines high strength with stable ductility, making it suitable for structural and load-bearing applications.

 

Specification of JIS G 3125 SPA-H Steel Plate

 

  • Thickness: ≤ 16 mmSPA-H

 

 

  • Width: ≤ 2000 mm

 

 

  • Length: Customized

 

 

  • Delivery condition: Hot rolled (HR)

 

Equivalent Grades

 

EN: S355J0WP (1.8945), S355JOWP

BS: WR50A / WR50B / WR50C

DIN: Fe510C1KI

GB: 09CuPCrNi-A

ISO: Fe355W-1A

 

Contact now

 

info-612-706

 

Q1: What is SPA-H Corten steel?

SPA-H is a Japanese standard weathering steel grade specified in JIS G 3125. It contains alloying elements such as copper, chromium, and nickel, which allow it to form a dense protective rust layer on the surface. This patina significantly slows down further corrosion and improves long-term durability in atmospheric environments.

 

Q2: What are the main advantages of SPA-H weathering steel?

The key advantages of SPA-H steel include excellent atmospheric corrosion resistance, high strength, and low maintenance cost. Unlike ordinary carbon steel, SPA-H does not require frequent painting or coating, which helps reduce lifecycle costs while maintaining a unique natural appearance.

 

Q3: Where is SPA-H Corten steel commonly used?

SPA-H steel is widely used in bridges, building structures, architectural façades, railway carriages, containers, air preheaters, and economizers. It is especially suitable for outdoor structures exposed to changing weather conditions for long periods.

 

Q4: Does SPA-H steel need painting or surface treatment?

In most outdoor applications, no additional painting is required. SPA-H naturally forms a stable rust layer after exposure to the atmosphere. However, in highly corrosive environments (such as marine or high-salt areas), additional surface protection may be recommended to extend service life.

 

Q5: How long does it take for SPA-H steel to form a stable patina?

Under normal atmospheric conditions, SPA-H steel typically forms a stable protective patina within 6 to 24 months