For customers procuring ASTM A588 Corten Steel, long-distance sea freight poses a high risk of premature rusting due to salt spray, high humidity, and seawater splashing. Proper packaging and transportation measures are critical to protecting the material's surface and ensuring subsequent performance. This article clarifies the core requirements for anti-rust during sea freight.

1. Core Packaging Requirements for Anti-Rust
Surface Pre-Treatment Before Packaging: Clean the surface of ASTM A588 sheets/plates to remove oil stains, dust, and loose rust. For unrusted or newly processed materials, apply a thin layer of temporary anti-rust oil (compatible with Corten Steel, easily removable) to form a primary anti-rust barrier.
Moisture-Proof & Salt-Proof Wrapping: Use multi-layer wrapping for each bundle: ① Inner layer: VCI (Volatile Corrosion Inhibitor) film, which releases corrosion-inhibiting gas to protect the surface from moisture and salt. ② Middle layer: Waterproof polyethylene film to block seawater and humid air penetration. ③ Outer layer: Heavy-duty woven plastic or jute cloth for physical protection against impact and splashing.
Sealing & Reinforcement: Seal all seams of the wrapping with waterproof adhesive tape to prevent air and water ingress. Use steel straps to reinforce the bundle (spacing ≤80cm) to avoid wrapping damage caused by shaking during transportation. For thick plates (≥10mm), add wooden pallets at the bottom to elevate the bundle above the container floor, preventing contact with accumulated water.

2. Key Transportation Requirements
Container Selection & Protection: Prioritize dry containers with intact seals and no water leakage. Place desiccant bags (2-3kg per 10m³) inside the container to absorb moisture. For bulk shipments, cover the top with a waterproof tarpaulin to prevent direct seawater splashing during loading/unloading and navigation.
Stowage & Fixing: Avoid stacking bundles too high (maximum 3 layers for thin sheets ≤8mm) to prevent crushing the lower packaging. Secure the bundles with container lashing straps to avoid collision and friction during ship swaying, which may damage the anti-rust wrapping.
Avoid Mixed Loading with Corrosive Goods: Do not load ASTM A588 with salt, chemicals, or other corrosive goods in the same container. Ensure the container is clean and free of residual corrosive substances before loading.

3. Post-Transportation Handling Suggestions
Timely Unpacking & Inspection: Unpack the bundles within 3-5 days after arrival at the destination. Inspect the surface for rust spots; if slight rust is found, clean it with a wire brush and apply anti-rust oil if necessary.
Removal of Temporary Anti-Rust Oil: Before use or further processing (e.g., welding, forming), remove the temporary anti-rust oil with a degreasing agent compatible with Corten Steel to avoid affecting the formation of the self-protective rust layer or welding quality.

In summary, the core of ASTM A588 sea freight anti-rust is "multi-layer moisture-proof packaging + proper container stowage". Following these requirements can effectively prevent premature rusting, ensuring the material's surface quality and performance meet project needs upon arrival.