S355J2WP high strength low alloy weathering Steel Plate

Oct 28, 2025 Leave a message

Products Description

 

S355J2WP is a weathering steel grade that offers high resistance to atmospheric corrosion. The thickness of the S355J2WP steel plate depends on the specific requirements and standards.

 

However, commonly available thicknesses range from 1.5 to 300 mm. The s355j2wp structural steel plates thickness is selected based on the intended application and the level of corrosion resistance required.

 

Thicker plates are often used in structural applications, while thinner plates are suitable for decorative or less demanding purposes.

 

S355J2WP steel plate specification

 

Width Length Thickness
1500 to 4050 mm 3000 to 15000 mm 6 to 200 mm
Standard Process Application
EN 10025 5 Hot Rolled (HR) architecture, smokestacks

 

Material s355j2wp Sheet mechanical properties

 

Grade Min Yield strength in different thickness Min tensile strength in different thickness Elongation in different thickness
  ≤
16
> 16
≤ 40
> 40
≤ 63
> 63
≤ 80
> 80
≤ 100
> 100
≤ 150
≤
3
> 3 ≤
100
> 100 ≤ 150 ≤ 1.5 > 2 ≤ 2.5 > 2.5 ≤ 3 > 3
≤ 40
> 40
≤ 63
> 63
≤ 100
> 100 ≤ 150
S355J2WP 355 345 – – – – 510-
680
470-
630
– 14 15 16 20 – – –

 

Corten steel s355j2wp sheet chemical properties

 

Grade Si
max
C max P max Mn
max
S max Cr max N
max
Cu max
S355J2WP 0.75 0.12 0.06-0.15 1.0 0.030 0.30-1.25 – 0.25-0.55

 

What are the unique properties of EN10025 S355J2WP plate ?

 

EN10025 S355J2WP plate forms a protective patina on its surface when exposed to the atmosphere which provides excellent resistance to atmospheric corrosion.

 

It a structurally robust and suitable for load-bearing applications.

 

The Corten steel s355j2wp plate adds a rustic and natural aesthetic.

 

The patina formation reduces the need for ongoing maintenance.

 

It has good weldability which allows ease of fabrication.

 

Contact now to get S355J2WP Quote

 

 