S355J2WP weathering steel plate equivalent grades

Oct 28, 2025 Leave a message

The number of S355J2WP weathering steel plate is 1.8946. And our company is the professional S355J2WP weathering steel plate supplier in China.

 

The standard of S355J2WP weathering steel plate is EN 10025-5: 2004 hot rolled products of structual steels. Technical delivery conditions for structural steels with improved atmospheric corrosion resistance.

 

Equivalent grades of S355J2WP weathering steel plate

EN

USA

AFNOR

EN

UNI

S355J2WP

A242Type1

E36WA4

Fe510D1KI

Fe510D1KI

 

This ensures that S355J2WP steel can be used globally in projects following different regional standards while maintaining consistent quality and performance.

 

Key Features and Advantages

Rust Resistance & Corrosion Resistance – Forms a self-protective patina to prevent further corrosion.

Life Extension – Significantly increases the service life of structures without frequent maintenance.

Thinning & Energy Saving – Allows for thinner structural sections while maintaining strength, reducing material usage and energy costs.

High Strength & Toughness – Suitable for demanding structural and industrial applications.

 

Applications

Structural Applications:

Bridges, towers, high-speed railways, vehicle bodies, and photovoltaic structures exposed to outdoor environments.

 

Industrial Equipment:

Manufacturing of containers, railway vehicles, oil derricks, seaport buildings, offshore oil platforms, and chemical and petroleum

 

equipment.

Particularly suitable for hydrogen sulfide-containing corrosive media, such as certain chemical tanks and process equipment.


With its combination of mechanical strength, atmospheric corrosion resistance, and long-term durability, S355J2WP weathering steel plate is an ideal material for heavy-duty structural, industrial, and marine applications where performance, maintenance reduction, and longevity are critical.

 