ASTM A709 Grade 50 is a high-strength low-alloy structural steel widely used in bridge fabrication and various engineering applications. This grade delivers a minimum tensile strength of 450 MPa and a yield strength of 345 MPa.

Thanks to alloying elements such as copper (Cu) and chromium (Cr), A709 Grade 50 steel plates demonstrate enhanced atmospheric corrosion resistance.
How Does A572 Grade 50 Differ From A709 Grade 50?
A572 Gr 50 generally contains a higher carbon level and slightly increased manganese content.
In contrast, A709 Gr 50 includes additional alloying ingredients designed to improve durability and performance.
A572 Grade 50 is preferred for general construction and everyday structural applications, while A709 Grade 50 is specifically intended for bridge-related structures and critical load-bearing components.
ASTM A709 Grade 50 Plate Specifications
Available Dimensions
| Thickness | Width | Length |
|---|---|---|
| 0.1875–3 in | 72–120 in | 240–1200 in |
Standard, Applications & Grades
| Standard | Application Fields | Grades |
|---|---|---|
| ASTM A709 | Bridge, building & construction sectors | 50, 50T, 50F |
Browse our real-time stock of ASTM A709-50 structural steel plates, all of which can be customized to meet project-specific requirements.
Available Types of A709 Grade 50 Plates
Standard Plate Options
ASTM A709 Grade 50 Plate
Width: 900–4800 mm
Thickness: 6–100 mm
Length: 3000–12000 mm
Cutting & Processing Services
Laser-cut plates
Flame-cut materials
Water-jet processed steel
Typical Applications of A709 Gr 50
Railway bridge structures
Pedestrian bridge components
Highway bridge girders
"Unable to source ASTM A709-50 in uncommon dimensions? Check our online inventory to reduce costs and verify product specifications."
Impact Strength Requirements for A709-50 Structural Plates
| Grade | Thickness (in) | Min. Longitudinal Value (ft-lbs) | Min. Avg. Energy (ft-lbs) | Zone 2 Temp | Zone 1 Temp | Zone 3 Temp |
|---|---|---|---|---|---|---|
| 50T | 2.01–3.00 | 15 | 20 | 40°F | 70°F | 10°F |
| 50T | 0.1875–2.00 | 10 | 15 | 40°F | 70°F | 10°F |
| 50F | 0.1875–2.00 | 20 | 25 | 40°F | 70°F | 10°F |
| 50F | 2.01–3.00 | 24 | 30 | - | - | - |
A709 Grade 50 Plate Equivalents
| EU (EN) | USA (ASTM) | Japan (JIS) | Germany (DIN/WNr) | Old EU |
|---|---|---|---|---|
| S355J2W (1.8965) | A709 Grade 50 | SMA50CP | WTSt52-3 | S355J2G2W |
Dimension Chart for A709 Gr 50 Plate
| Grade | Width (in) | Thickness (in) | Length (in) |
|---|---|---|---|
| 50F | 72–120 | 2.51–3.00 | 240–1200 |
| 50T | 72–120 | 0.1875–3.00 | 240–1200 |
| 50 | 72–120 | 0.1875–3.00 | 240–1200 |
| 50F | 72–120 | 0.1875–2.50 | 240–1200 |
Mechanical Properties of ASTM A709-50 Plates
| Grade | Thickness (in) | Elongation 2" (%) | Tensile (ksi) | Yield (ksi) | Elongation 8" (%) |
|---|---|---|---|---|---|
| 50T | 0.1875–3.00 | 21 | 65 | 50 | 18 |
| 50 | 0.1875–3.00 | 21 | 65 | 50 | 18 |
| 50F | 0.1875–3.00 | 21 | 65 | 50 | 18 |
Chemical Composition of A709 Grade 50
The steel may include manganese up to 1.35%, carbon capped at 0.23%, and sulfur/phosphorus both limited to 0.030%. Depending on the type, alloying elements such as copper (min 0.20%), silicon (max 0.40%), niobium, and vanadium may be present to enhance strength and corrosion resistance.
What Should You Check Before Purchasing an A709 Grade 50 Plate?
Request mill test reports (MTC) to verify compliance with ASTM A709 Grade 50 requirements.
Consider the intended end-use and confirm the grade matches your structural needs.
Select the correct size and thickness based on load calculations.
For harsh outdoor environments, choose A709 Grade 50 Type 2 for better corrosion resistance.
Buy from a certified, reputable supplier that follows recognized quality standards.
Confirm lead time and delivery schedules to keep your project on track.
Difference Between A709 Grade 50 and 50W
A709 Grade 50 contains higher amounts of carbon and manganese.
A709 Grade 50W includes additional alloying elements responsible for weathering resistance.
Grade 50W forms a protective oxide layer, eliminating the need for external coatings in many atmospheric conditions.
Quality Tests Used for A709 Grade 50 Plates
Chemical analysis to verify alloy composition
Tensile testing for evaluating yield, tensile strength, and elongation
Charpy V-notch tests to measure impact resistance at low temperatures
Ultrasonic examination to detect internal flaws
Visual inspections for surface irregularities