What is A588 Grade C Steel Plate?
Gnee ASTM A588 Grade C steel plate is a high-strength, low-alloy structural steel with enhanced atmospheric corrosion resistance, designed for structural shapes such as angles, channels, beams, plates, and bars.

It is widely used in welded bridges, buildings, and other structures where weight savings, durability, and long service life are important.
Key Features:
Minimum yield strength of 345 MPa for thickness up to 100 mm.
Can be produced up to 200 mm thickness in our facilities.
Excellent atmospheric corrosion resistance, substantially better than ordinary carbon structural steel.
Can be delivered in various forms: hot-rolled, cold-rolled, normalized, quenched and tempered, TMCP (Thermo-Mechanical Control Process), electroslag remelting, and tested with HIC.
Delivery Conditions
Hot Rolled / Cold Rolled
Normalized / Quenched / Tempered
Thermo-Mechanical Control Process (TMCP)
Electroslag Remelting (ESR)
HIC Test Certified
Grade & Specification
| Item | Specification |
|---|---|
| Product | Steel plate, steel sheet, carbon steel sheet |
| Standard | ASTM A588, A242 |
| Material | Corten A, Corten B, S355J0WP, S355J0W, S355J2W, A588 Grade A/B/C, A242 Type 1, SA588 Grade A/B/C |
| Thickness | 6 mm – 200 mm |
| Width | 1500 mm – 4050 mm |
| Length | 3000 mm – 15000 mm |
| Surface | Black painted, PE coated, galvanized, color coated, anti-rust varnished, anti-rust oiled, checkered |
| Packaging | Standard export package suitable for all transport modes, or as required |
| Export To | Saudi Arabia, Kuwait, Qatar, Pakistan, UAE, Turkey, Kazakhstan, Greece, Singapore, Thailand, Indonesia, Vietnam, South Africa, South America, Brazil, India, Australia, Egypt |
Chemical Composition (% Max)
| Element | C | Si | Mn | P | S | Cu | Ni |
|---|---|---|---|---|---|---|---|
| Max % | 0.20 | 0.15–0.50 | 0.75–1.35 | 0.04 | 0.05 | 0.40–0.70 | 0.50 |
Carbon Equivalent Formula:
Ceq=C+Mn6+Cr+Mo+V5+Ni+Cu15%Ceq = C + \frac{Mn}{6} + \frac{Cr+Mo+V}{5} + \frac{Ni+Cu}{15} \%Ceq=C+6Mn+5Cr+Mo+V+15Ni+Cu%
Mechanical Properties
| Thickness (mm) | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) |
|---|---|---|---|
| ≤100 | 485 | 345 | 21 |
| 100–125 | 460 | 315 | 18 |
| 125–200 | 435 | 290 | 18 |
Applications
Due to its superior strength, durability, and atmospheric corrosion resistance, A588 Grade C steel is widely used in the following applications, with supporting data:
Bridge Construction and Structural Frameworks:
Tensile strength up to 485 MPa (for thickness ≤100 mm) and yield strength ≥345 MPa, suitable for supporting loads exceeding 50 tons per beam.
Commonly used in welded bridges with spans up to 500 meters, providing long-term structural reliability.
Retaining Walls, Facades, and Urban Infrastructure:
Thickness range 6–200 mm, width 1500–4050 mm, length 3000–15000 mm, ideal for large-scale urban projects.
Atmospheric corrosion resistance ensures material loss <0.02 mm/year in industrial or coastal environments, extending service life to 50+ years.
Fences, Sculptures, Industrial Containers, and Urban Furniture:
Durable in outdoor exposure with minimal maintenance; the self-protecting rust layer reduces upkeep costs by 30–40% compared to conventional carbon steel.
Suitable for industrial containers carrying up to 20 tons of material, sculptures and urban furniture exposed to weather and pollutants.
Outdoor Architectural and Industrial Applications:
Applicable in marine, industrial, and high-humidity environments, with corrosion resistance 2–3 times better than ordinary carbon structural steels.
Ensures long-term aesthetics and structural integrity, supporting projects with decades-long lifecycle requirements.