Products Description
Q310GNH, Q295NH, and Q355NH weathering steel plates are low-alloy high-strength steels (Weathering Steel) with excellent atmospheric corrosion resistance and high mechanical performance.
Positioned between ordinary carbon steel and stainless steel, these steels are alloyed with small amounts of copper, nickel, chromium, and trace elements such as phosphorus, sulfur, and titanium.

Under natural exposure, they form a dense oxide protective layer approximately 50–100 μm thick, which significantly reduces the corrosion rate, giving a service life 2–5 times longer than ordinary carbon structural steel.
These steels not only reduce structural weight and improve reliability but also save materials and resources, making them ideal for modern large-scale engineering projects requiring high strength, durability, and low maintenance.
Chemical Composition
| Element | C | Si | Mn | P | S | B | Mo | V |
|---|---|---|---|---|---|---|---|---|
| Content | 0.08–0.14 | 0.40–0.60 | 1.20–1.50 | ≤0.035 | ≤0.010 | ≤0.005 | 0.15–0.30 | 0.03–0.08 |
Mechanical Properties (Thickness T ≤ 65 mm)
| Property | Value |
|---|---|
| Yield Strength | ≥ 690 MPa |
| Tensile Strength | 760–895 MPa |
| Elongation | ≥ 18% |
| Cold Bending | 180° without cracking |
| Impact Toughness (Charpy V-notch, 20°C) | ≥ 27 J |
Typical Applications
Bridges and Large Steel Structures: Main beams, deck panels, towers, and supporting structures; capable of withstanding loads of 200–500 kN/m², suitable for highway and railway bridges.
Pressure Vessels and High-Pressure Tanks: Suitable for internal working pressures ≤30 MPa, widely used in chemical, power, and oil & gas storage facilities.
Ships and Marine Structures: Can be used in coastal and marine environments for 20–25+ years, commonly for ship hulls, dock panels, and offshore platforms.
Vehicles and Transportation Equipment: Railway freight cars, container bases, and vehicle frames, enhancing durability while reducing weight.
Landscape Architecture and Building Facades: Planters, flower beds, fences, decorative walls, and building cladding, with naturally formed reddish-brown patina.
Other Performance & Design Parameters
Temperature Resistance: Suitable for structures and flue systems at ambient temperature to 400°C.
Corrosion Rate: 0.01–0.02 mm/year in normal atmosphere; ~0.03 mm/year in coastal environments.
Weldability: Compatible with SMAW, GMAW, FCAW, and other common welding methods, crack-free after welding.
Fabrication: Can be cut, punched, bent, and machined without special pre-treatment.
Product Advantages
High Strength, Reduced Weight: Can reduce structural weight by 15–25% compared to ordinary carbon steel, saving steel and construction costs.
Long-Term Weather Resistance: Service life 20–30 years in urban/industrial environments; 25+ years in coastal/high-humidity areas.
Low Maintenance Costs: No regular painting or corrosion protection required.
Excellent Weldability and Workability: Suitable for complex and large-scale structural applications.
Natural Aesthetic Appeal: Red-brown patina forms naturally over time, combining decorative effect with structural performance.