Elongation (plastic deformability) of Q460NH increases as temperature rises, which is typical for structural steels. Below is a general summary based on industry and material test data for similar high-strength weathering steels:
1. Room temperature (20°C)
Elongation A: typically ≥ 18% (standard minimum requirement)
Actual production values often reach 20%–24%
Good balance of strength and ductility for cold forming and welding.
2. 100°C – 200°C
Elongation slightly increases to around 22%–26%
Material becomes marginally softer and more ductile
No significant loss of structural stability.

3. 200°C – 300°C
Elongation continues rising noticeably, often 25%–30%
Ductility improves while strength decreases
The material becomes easier to deform but is not suitable for load-bearing parts due to strength reduction.
4. 300°C – 400°C
Elongation can exceed 30%
Significant softening and plastic deformation occur easily under load
Creep deformation becomes prominent; Q460NH is not intended for use in this range.

5. Above 400°C
Elongation rises further, but the material loses effective structural strength
Microstructure deteriorates; long-term service leads to progressive damage.