In addition to annealing, tempering and normalizing are two practical thermal treatment methods to improve the ductility/elongation of SPA-H weathering steel-both relieve internal stresses, modify the steel's microstructure, and restore formability, with distinct application scenarios based on the steel's initial processing state (cold-rolled, welded, or hot-rolled) and performance requirements. Below are the specific parameters, mechanisms, and effects of each method:

info-569-535

1. Tempering (Ideal for Post-Cold-Forming/Cold-Rolled SPA-H)

 

Core Purpose: Alleviate work hardening in cold-rolled or cold-formed SPA-H, improve ductility to avoid cracking during secondary shaping (bending, stamping), while retaining most cold-rolled strength gains.

Standard Parameters: Heat to 550–650°C (below austenitization), hold for 1–2 hours (or 1 min/mm of thickness for thick gauges), then cool slowly in air or furnace.

Mechanism: Reduces the hardness of work-hardened microstructures, relieves residual compressive stresses from cold processing, and softens brittle martensite/bainite phases (if present) without full grain recrystallization.

Ductility Improvement: Raises elongation at break by 5–8 percentage points for cold-rolled SPA-H (from ≤15% to ~20–23%); slightly improves toughness while only a 5–10% reduction in yield strength.

Best For: Thin/medium cold-rolled SPA-H gauges (1.6–25 mm) that need post-rolling forming and a balance of ductility and strength.

info-233-223

2. Normalizing (Ideal for Hot-Rolled/Welded SPA-H or Over-Worked Cold-Rolled SPA-H)

 

Core Purpose: Refine grain structure, eliminate residual stresses from rolling/welding, and balance ductility, toughness and strength for structural SPA-H components.

Standard Parameters: Heat to 880–920°C (above austenitization), hold for 2–3 min/mm of thickness (minimum 30 mins for thin gauges), then cool in still air.

Mechanism: Transforms coarse/uneven grains (from hot rolling) or distorted grains (from heavy cold rolling) into fine, equiaxed ferrite-pearlite grains via full austenitization and uniform air cooling; fully relieves internal stresses (80–90% stress elimination).

Ductility Improvement: For hot-rolled SPA-H: increases elongation by 8–12 percentage points (from ≥20% to ≥22–24%); for cold-rolled SPA-H: restores elongation to 18–20% (reversing excessive work hardening).

Best For: Thick SPA-H gauges (>25 mm), welded structural components, or cold-rolled SPA-H with severe work hardening that needs comprehensive microstructure optimization.

info-565-551