Are there any other factors that affect the impact toughness of Q355NH besides temperature?

Mar 16, 2026 Leave a message

Many factors strongly influence the impact toughness of Q355NH weathering steel, even at the same test temperature. Below is a detailed, professional explanation you can use directly for technical reports or client communication.

1. Steel Plate Thickness

Thinner plates (≤ 16 mm)Finer grain structure, more uniform composition → higher impact toughness.

Thicker plates (> 16 mm)Slower cooling during production → coarser internal grains, possible center segregation → lower toughness, especially in the mid-thickness region.

Standard impact values often decrease as thickness increases.

2. Chemical Composition

Key elements directly affect toughness:

Carbon (C) contentHigher C increases strength but reduces toughness and raises cold-crack sensitivity.

Manganese (Mn)Improves toughness within the standard range; excess Mn can cause segregation.

Phosphorus (P) & Sulfur (S)Both are harmful impurities that cause grain boundary embrittlement.Q355NH controls P ≤ 0.030% and S ≤ 0.025% to ensure basic toughness.

info-542-355

Weathering alloys (Cu, Cr, Ni)Ni slightly improves low-temperature toughness;Excess Cr/Cu may slightly reduce toughness if not balanced.

3. Heat Affected Zone (HAZ) from Welding

Welding heat changes the microstructure near the weld.

Overheated zone: grain coarsening → sharply reduced toughness.

Unmatched filler metal, excessive heat input, or lack of preheatingcan lead to hardening in the HAZ and lower impact energy.

Weld defects (porosity, cracks, inclusions) also reduce effective toughness.

4. Microstructure & Production Process

Hot rolling and controlled coolingRefined grains = higher toughness.

Normalizing or controlled rolling processProduces more uniform ferrite–pearlite structure and better toughness.

Untreated or rapidly cooled material may have higher hardness and lower toughness.

info-331-249

5. Strain Hardening & Cold Working

Bending, shearing, stamping, or mechanical deformation causes strain hardening.

Severe cold working increases strength but reduces plasticity and impact toughness.

Sharp notches, scratches, or edge defects act as stress concentrators and lower actual impact resistance.

6. Aging & Service Environment

Long-term outdoor exposureStable patina does not harm toughness, but

Local pitting corrosion reduces effective cross-section and creates stress concentrations.

In high-temperature or long-term cyclic loading environments, material aging may gradually reduce toughness.

7. Loading Rate & Notch Effect

Impact toughness is highly sensitive to loading speed; faster impact = lower absorbed energy.

Sharp notches (from welding, cutting, corrosion pits) drastically reduce toughness compared to smooth surfaces.

info-247-230