Corten B Hot Rolled Atmospheric Corrosion Steel Sheet

Nov 05, 2025 Leave a message

What Corten B Is and Which Standards Cover It

Corten B is the common trade designation for a hot rolled, high strength low alloy steel developed for structural service in aggressive outdoor atmospheres. In specification terms it corresponds to ASTM A588/A588M Grade A in the United States and to the S355J0W and S355J2W weathering grades of EN 10025-5 in Europe, with JIS G3114 covering the equivalent Japanese grades. All of these designations describe the same underlying idea: a structural steel whose alloy content lets the surface form a protective oxide layer instead of shedding rust.

The material is supplied as hot rolled plate and coil, and is also available as sections and hollow sections. It is intended for welded, bolted and riveted construction, and in most cases it is used bare without a protective coating.

Chemical Composition and the Corrosion Mechanism

The weathering behaviour comes from deliberate alloy additions rather than from a surface treatment. A typical Corten B heat analysis is limited as shown below, in mass percent.

Element C max Mn P max S max Si Cu Cr Ni max V
Corten B, ASTM A588 Grade A basis 0.19 0.80-1.25 0.04 0.05 0.30-0.65 0.25-0.40 0.40-0.65 0.40 0.02-0.10

Copper is the primary element that suppresses atmospheric attack, chromium strengthens the oxide film, and nickel improves toughness and helps the layer adhere. Silicon supports oxide formation, while vanadium contributes strength through grain refinement. Other grades within ASTM A588 and the higher-phosphorus grades of EN 10025-5 vary these ranges, so acceptance should always be checked against the specific grade on the order.

In service the surface first discolours to orange, then over roughly 6 to 24 months forms a dense brown layer. Because that layer is compact, it restricts the access of oxygen and moisture to the underlying steel, and long-term corrosion rates reported in technical literature for weathering steels in suitable atmospheres are far lower than those of unprotected carbon steel in the same exposure.

Mechanical Properties and Delivery Conditions

Property Requirement for plate up to 100 mm
Minimum yield strength 345 MPa
Minimum tensile strength 485 MPa
Minimum elongation About 18 to 21 percent, depending on thickness
Impact testing J0 at 0 C or J2 at -20 C, according to the ordered grade

The thickness range for plate is commonly 3 mm to 150 mm, and heavier material is arranged case by case. Delivery conditions available from production include hot rolled, cold rolled, normalized, quenched and tempered, and thermomechanically controlled rolling. Additional processing routes such as remelting or hydrogen induced cracking testing are offered where a project specifies them, although these are unusual for ordinary weathering applications. Ceramic or ultrasonic testing of plate follows EN 10160 when required, dimensional tolerances follow EN 10029, and certificates are issued to EN 10204 type 3.1.

Welding, Cutting and Forming

Corten B welds with the same processes used for other low-alloy structural steels, provided the consumables and heat input are selected properly. Carbon equivalent is controlled to keep weldability within normal fabrication practice, and electrodes with a low hydrogen content are used for thick sections and restrained joints. Procedures are qualified to EN ISO 15614-1 and welders to EN ISO 9606-1 where European standards govern the project.

Cutting is carried out by plasma, laser, oxy-fuel or abrasive methods as thickness dictates, and thermally cut edges are dressed where fatigue or wet service demands it. The material bends and rolls to normal structural radii at ambient temperature. For bolted connections, fasteners of a matching strength class are used and should be galvanically compatible with the weathering steel; where dissimilar metals meet, an isolating washer or coating is required to avoid accelerated local attack. Drilling and machining resemble other low-alloy plate grades, with slightly higher tool wear than plain carbon steel because of the copper content.

Applications and Quality Control

Typical uses include bridge girders and parapets, rail wagons, shipping containers, chimneys and ductwork, tanks and bins, transmission poles, industrial platforms, vehicles and heavy outdoor equipment, and architectural cladding where the weathered appearance is part of the design.

The material suits open, well-ventilated exposures with alternating wet and dry cycling. It is not suitable for permanent immersion, buried service or chloride-rich coastal atmospheres, where the oxide layer cannot stabilise and corrosion proceeds as it would in ordinary steel. Where those conditions cannot be avoided, either a protective coating system or a different material should be selected.

Quality control covers heat analysis, tensile and impact testing on each heat, dimensional and flatness checks to EN 10029, and surface inspection against EN 10163 before despatch. Heat numbers should be traceable from the certificate to the piece delivered, because the corrosion performance of the product depends entirely on the alloy content that the certificate records.

Frequently Asked Questions

Q: What is Corten B equivalent to?

A: It corresponds to ASTM A588/A588M Grade A and to EN 10025-5 grades such as S355J0W and S355J2W.

Q: What are its yield and tensile strengths?

A: A minimum yield strength of 345 MPa and a minimum tensile strength of 485 MPa for plate up to 100 mm thick.

Q: Why does the steel not need painting?

A: Copper, chromium and nickel let the surface form a compact oxide layer that limits further attack, so bare use is possible in suitable atmospheres.

Q: Can Corten B be welded?

A: Yes, with qualified procedures and low-hydrogen consumables, and with heat input controlled to suit the plate thickness.

Q: Is it suitable for marine conditions?

A: No. Chloride-rich atmospheres prevent the protective layer from stabilising, so coating or another material is required.

Q: What thickness range is available?

A: Commonly 3 mm to 150 mm, with heavier plate and non-standard sizes arranged against the order.