A423 Gr1 HFW electric resistance welded pipe

Nov 19, 2026 Leave a message

ASTM A423 Grade1 HFW Electric Resistance Welded Pipe

ASTM A423 Grade 1 HFW electric resistance welded pipe is a low-alloy steel tube manufactured in accordance with ASTM A423/A423M for pressure-containing components, economizers, and industrial applications requiring atmospheric corrosion resistance. The material contains 0.20–0.60% copper, 0.24–1.31% chromium, and 0.20–0.70% nickel, with a maximum carbon content of 0.15%.

 

Manufactured through high-frequency welding (HFW), ASTM A423 Gr.1 electric resistance welded steel pipe is formed from steel strip or coil, with longitudinal edges joined by electrical resistance heating and mechanical pressure. The finished tubing is supplied in normalized or other specified heat-treated conditions to meet the applicable standard requirements.

 

As a manufacturer and supplier of ASTM A423 Grade 1 electric welded tubing, we provide customized outside diameters, minimum wall thicknesses, cutting lengths, material inspection, and export packaging for industrial buyers and engineering projects.

ASTM A423 Grade 1 HFW electric resistance welded pipe
A423 Grade 1 HFW electric resistance welded pipe

What Is ASTM A423 Grade 1 Low Alloy Steel?

ASTM A423 Grade 1 is a copper-chromium-nickel-containing low-alloy steel designed for tubular applications where atmospheric corrosion resistance is required.

 

Unlike ordinary carbon steel, ASTM A423 Gr.1 contains controlled quantities of copper, chromium, and nickel. These elements contribute to the formation and stability of corrosion products on the steel surface under suitable atmospheric exposure conditions.

 

ASTM A423 Grade 1 steel is used in equipment exposed to atmospheric conditions and industrial environments where the material's corrosion characteristics must be considered during material selection.

 

ASTM A423 Grade 1 HFW Electric Resistance Welded Pipe Manufacturer and Supplier

Our ASTM A423 Grade 1 HFW electric resistance welded pipe is manufactured using a continuous forming and high-frequency resistance welding process.

 

During production, steel strips are fed into a forming system and gradually shaped into a cylindrical tube. High-frequency electrical current heats the adjoining strip edges, and squeeze rolls apply pressure to complete the longitudinal weld without adding filler metal.

The main manufacturing stages include:

 

Raw Material Preparation: ASTM A423 Grade 1 steel coils are inspected for chemical composition, surface quality, and dimensional consistency.

Strip Slitting: Steel coils are slit into strips according to the required pipe outside diameter and wall thickness.

Roll Forming: The strips pass through forming rolls to create an open tubular shape.

High-Frequency Welding: Electrical resistance heating and squeeze pressure join the longitudinal edges.

Weld Seam Treatment: The weld seam is inspected and processed according to the manufacturing procedure and applicable requirements.

Sizing and Straightening: Sizing rolls control the finished outside diameter and straightness.

Heat Treatment: Normalizing or other required heat treatment is applied to achieve compliance with ASTM A423/A423M.

Cutting and Inspection: Finished electric welded tubing is cut to the specified length and subjected to dimensional and mechanical testing.

A423 Gr.1 ERW Corten Steel Tubes
A423 Gr.1 electric resistance welded pipes
A423 Gr.1 electric welded steel tubing
A423 Gr.1 erw round steel pipe

ASTM A423 Gr.1 Electric Resistance Welded Steel Pipe Specification

Parameter

Specification

Standard

ASTM A423/A423M

Grade

ASTM A423 Grade 1 / ASTM A423 Gr.1

Product Type

Electric Resistance Welded Steel Tube

Manufacturing Proces

HFW (High-Frequency Welding)

Steel Classification

Low-Alloy Steel

Outside Diameter

21-76 mm (standard commonly supplied range)

Wall Thickness 

1.5-4.0 mm (standard commonly supplied range)

Length 

Customized

Manufacturing Finish

Hot Finished / Cold Finished

Heat Treatment

Normalized or other specified heat treatment

Weld Type 

Longitudinal Weld

End Finish 

Plain End / Beveled End (as agreed)

Certification

EN 10204 3.1 MTC (upon order agreement)

 

Chemical Composition of ASTM A423 Grade 1 Electric Welded Pipes

The chemical composition of ASTM A423 Grade 1 is controlled according to the requirements of ASTM A423/A423M Table 1.

Element

Chemical Composition (%)

Carbon (C)

≤0.15

Manganese (Mn)

≤0.55

Phosphorus (P)

0.06–0.16

Sulfur (S)

≤0.060

Silicon (Si)

≥0.10

Copper (Cu)

0.20–0.60

Chromium (Cr)

0.24–1.31

Nickel (Ni)

0.20–0.70

Molybdenum (Mo)

No specified requirement

Antimony (Sb)

No specified requirement

 

Mechanical Properties of ASTM A423 Gr.1 Electric Resistance Welded Tubing

ASTM A423 Grade 1 electric resistance welded tubing must meet the specified tensile properties and hardness requirements.

Mechanical Property 

ASTM A423 Grade 1 Requirement

Tensile Strength 

≥415 MPa (60 ksi)

Yield Strength 

≥255 MPa (37 ksi)

Elongation 

≥25%

Brinell Hardness

≤170 HBW

Rockwell Hardness

≤87 HRBW

The elongation requirement is based on a 50 mm (2-inch) gauge length. For applicable longitudinal strip specimens with wall thickness below 8 mm, the standard provides an elongation adjustment of 1.25 percentage points for each 0.8 mm reduction below the reference thickness.

 

Why Choose ASTM A423 Grade 1 HFW Electric Welded Tubing?

ASTM A423 Grade 1 HFW electric welded tubing combines controlled low-alloy chemistry with a longitudinal electric-resistance-welded structure. Its selection for industrial equipment is based on the following material and manufacturing characteristics.

 

1. Copper-Chromium-Nickel Alloy Composition

The copper content of 0.20–0.60%, chromium content of 0.24–1.31%, and nickel content of 0.20–0.70% distinguish ASTM A423 Gr.1 electric resistance welded steel pipe from ordinary carbon steel tubing.

 

These alloying elements contribute to atmospheric corrosion resistance. However, the actual corrosion rate must be evaluated against the operating environment and exposure conditions.

 

2. Longitudinal HFW Welding Structure

The HFW manufacturing process produces a continuous longitudinal weld along the pipe body. The process does not require additional welding filler metal and is suitable for continuous production of straight electric welded pipes.

 

Weld quality is verified through the applicable inspection procedures, including flattening, reverse flattening, hydrostatic testing, or nondestructive electric testing.

 

3. Defined Mechanical Properties

ASTM A423 Grade 1 electric resistance welded steel tubing requires a minimum tensile strength of 415 MPa and a minimum yield strength of 255 MPa, with a minimum elongation of 25%.

 

These values provide measurable criteria for evaluating the material's suitability for pressure-containing tubular applications.

 

4. Flexible Manufacturing Dimensions

The standard commonly covers outside diameters from 12.7 mm to 127 mm and minimum wall thicknesses from 0.9 mm to 12.7 mm. Other dimensions can be considered subject to agreement and compliance with the standard.

 

ASTM A423 Grade 1 Electric Resistance Welded Steel Pipe Applications

ASTM A423 Gr.1 electric resistance welded steel pipe is primarily used in industrial equipment requiring low-alloy steel tubing with specified mechanical properties and corrosion resistance. Typical applications include:

Economizer Tubes

Used in boiler economizers to transfer heat from flue gas to feedwater. The tubing operates as part of a pressure-containing heat recovery system.

 

Industrial Heat Exchangers

Used in heat exchanger assemblies where tube material selection is based on working pressure, temperature, fluid composition, and corrosion conditions.

 

Petrochemical and Chemical Processing Equipment

Used in tubular components exposed to industrial atmospheric or process environments where the chemical compatibility of ASTM A423 Grade 1 steel has been verified.

A423 Gr.1electric resistance welded pipe
A423 Gr.1 electric welded pipes
A243 Grade 1 electric welded pipes

ASTM A423 Grade 1 Electric Welded Tubing vs. Ordinary Carbon Steel Pipe

Comparison

ASTM A423 Grade 1

ASTM A53 Grade B

Material Type

Low-Alloy Steel

Carbon Steel

Copper

0.20–0.60%

-

Chromium

0.24–1.31%

-

Nickel

0.20–0.70%

-

Minimum Tensile Strength

415 MPa

415 MPa

Minimum Yield Strength

255 MPa

240 MPa

Main Applications

Economizers and corrosion-resistant tubular applications

General pressure and structural piping

 

ASTM A423 Grade 1 Electric Resistance Welded Tubing Inspection and Testing

Quality inspection is an essential part of manufacturing ASTM A423 Grade 1 electric resistance welded tubing. Testing is performed according to ASTM A423/A423M and the applicable general requirements of ASTM A450/A450M.

Inspection Item 

Testing Method

Chemical Analysis

Heat Analysis / Product Analysis

Tensile Test

ASTM A450/A450M

Hardness Test

Brinell / Rockwell

Flattening Test

Flattening Test

Flange Test

Flange Test

Reverse Flattening Test

Reverse Flattening Test

Hydrostatic Test

Hydrostatic Pressure Test

Nondestructive Electric Test

Eddy Current / Other Qualified NDE

Dimensional Inspection

OD / Wall Thickness / Length

Visual Inspection

Surface and Weld Examination

For each finished tube, hydrostatic testing or nondestructive electric testing is performed as required by the standard and the agreed purchase requirements. The purchaser should specify the required test option when placing the order.

A423 GR.1 Straight seam welded pipe
A423 GR.1 erw welded steel pipe
A423 GR.1 erw round steel tube

ASTM A423 Gr.1 Electric Resistance Welded Steel Tubing Packaging and Certification

To protect ASTM A423 Grade 1 electric resistance welded steel pipes during storage and international transportation, suitable packaging is selected according to pipe dimensions, surface condition, and shipping requirements.

 

Our export packaging options include:

  • Bundling: Pipes are bundled using steel straps with protective supports.
  • End Protection: Plastic or metal end caps can be fitted to reduce damage and contamination.
  • Surface Protection: Anti-rust oil or protective wrapping can be applied when specified.
  • Wooden Crates: Export-grade wooden cases can be arranged for smaller-diameter or customized tubing.
  • Container Loading: Bundles are secured to minimize movement during transportation.

 

Available documentation can include:

  • Mill Test Certificate (MTC).
  • Chemical Composition Report.
  • Mechanical Test Report.
  • Dimensional Inspection Report.
  • Nondestructive Testing Report.
  • Third-Party Inspection Documents (SGS, BV, TUV), subject to agreement.
A423 GR.1 electric resistance welded pipe
ASTM A423 Gr.1 Electric Resistance Welded Steel Tubing

ASTM A423 Grade 1 Electric Resistance Welded Pipe Manufacturer

As a professional steel pipe supplier, we support the procurement of ASTM A423 Grade 1 HFW electric resistance welded pipes for boiler, economizer, heat exchanger, and industrial equipment manufacturers.

 

We can discuss customized outside diameters, minimum wall thicknesses, fixed lengths, inspection requirements, and packaging specifications according to your project drawings and purchase requirements.

 

To receive an accurate quotation for ASTM A423 Gr.1 electric resistance welded tubing, please provide:

Grade and Standard: ASTM A423 Grade 1 / ASTM A423/A423M.

Outside Diameter (OD): Required diameter in mm or inches.

Wall Thickness (WT): Required minimum wall thickness.

Length: Fixed length or random length.

Quantity: Required quantity in metric tons, pieces, or meters.

Inspection Requirements: Hydrostatic Test, Eddy Current Test, or Third-Party Inspection.

Delivery Destination: Country and port of destination.

 

We welcome inquiries from distributors, EPC contractors, boiler manufacturers, and industrial equipment suppliers.