EN10025-5 S355J0WP Hot Rolled Weathering Steel Sheet

Sep 05, 2025 Leave a message

S355J0WP Steel Description

 

S355J0WP is a structural weathering steel which is also referred to as atmospheric corrosion resistant steel. The main alloying elements are chromium nickel and copper with added phosphorous which gives it excellent self protecting qualities.

 

info-419-414

 

As the steel reacts with elements in the atmosphere, the material forms a layer of rust over time which in essence protects the steel from corrosion.

 

S235J2W Steel Delivery State

 

Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.

 

S355J0WP steel application

 

S355J0WP (which is an equivalent grade to Corten A) provides a long lasting and economic structural steel solution for use in applications such as steel bridges stack gas applications and in steel sculptured buildings due to the material's aesthetically pleasing finish.

 

Moreover, S355J0WP steel with improved atmospheric corrosion resistance has a wide range of applications: architecture, smokestacks, fabrication, freight wagons, silos, pylons etc..

 

S355J0WP

 

S355J0WP steel chemical composition by [%]

 

C % Mn % Cr % Si % CEV % S %
Max 0.12 Max 1 0.3-1.25 Max 0.75 Max 0.52 Max 0.035
Cu % P % N %      
0.25-0.55 0.06 - 0.15 Max 0.009      

Method of deoxidation FN = rimming steels not permitted.
For long products the P and S content can be 0.005% higher
The S355J0WP steels may show a Ni content of max. 0,65 %.


The max. value for nitrogen does not apply if the chemical composition shows a minimum total Al content of 0,020 % or if sufficient other N binding elements are present. The N binding elements shall be mentioned in the inspection document

 

S355J0WP steel Mechanical properties

 

Grade Min. Yield Strength Mpa Tensile Strength MPa Impact
S355J0WP Nominal Thickness (mm) Nominal Thickness (mm) degree J
Thick mm ≤16 >16
≤40
>40
≤63
>63
≤80
>80
≤100
>100
≤150
≤3 >3 ≤100 >100 ≤150 0 27
S355J0WP 355 345 …. …. …. …. 510-680 470-630 ….

The tensile test values given in the table apply to longitudinal samples; in case of strip and sheet steel of widths of ≥600 mm they apply to transverse samples.

 

If S355J0WP mechanical properties have been significantly modified by heavy coldforming, either stress relief annealing or normalised may be applied. Normalised should also be applied following hotforming outside of the temperature range of 750 - 1.050 °C and after overheating.

 

S355J0WP Steel Services

 

Cutting, Painting, shot blast, and The third party inspection in DNV, BV, LR, GL, ABS, CCS , SGS, and others in super thick ship steel plate.

 

One-Stop Weathering Steel Solutions for Diverse Project Needs

 

At Gnee, we provide full-process corten steel solutions including design, fabrication, surface treatment, and global shipping. Whether you're building a facade, a garden structure, or an industrial component, we deliver with speed, quality, and flexibility.

 

Our service highlights:

 

 Drawing optimization and custom design

 

 Precision fabrication with strict quality control

 

 Various surface finishes: pre-rusted, painted, or anti-corrosion

 

 Export-grade packaging and reliable worldwide logistics

 

 Full technical support before and after sales

 

One supplier for everything – streamlined and efficient project delivery.

 

Contact now to get S355J0WP Quote