S355J0W Steel Description
S355J0W steel is a weather resistant steel which could more accurately be termed as an "Atmospheric Corrosion Resistant Steel" and often referred to as Corten-B steel.

Weathering means that due to S355J0W steel chemical compositions, S355J0W steel chemical composition can increase resistance to atmospheric corrosion compared to other steels. This is because it forms a protective layer on S355J0W steel surface under the influence of the weather.
S355J0W steel Deliver condition
Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.
S355J0W steel Application range
The S355J0W steels are used for various types of welded, bolted and riveted constructions e.g. steel frame structures, bridges, tanks and containers, exhaust systems, vehicles and equipment constructions and so on.

S355J0W steel Chemical composition (%)
| C | Si | Mn | P | S | Cr | N | Cu | CEV |
|
max 0.16 |
Max 0.5 |
0.5 - 1.5 |
max 0.035 |
Max 0.035 |
0.4 -0.8 |
max 0.009 |
0.25-0.55 |
Max 0.52 |
|
Note: |
||||||||
S355J0W steel mechanical property
| Nominal thickness (mm) | to 16 | 16-40 | 40-63 | 63-80 | 80-100 | 100-150 |
| ReH - Minimum yield strength (MPa) | 355 | 345 | 335 | 325 | 315 | 295 |
| Nominal thickness (mm) | To 3 | 3-100 | 100-150 | |||
| Rm -Tensile strength (MPa) | 510-680 | 470-630 | 450-600 | |||
| Nominal thickness (mm) | 3-40 | 40-63 | 63-100 | 100-150 | ||
| A - Minimum elongation Lo = 5,65 √ So (%) | 22 | 21 | 20 | 18 | ||
| Nominal thickness (mm) | 1.5 - 2 | 2-2.5 | 2.5-3 | |||
| A - Minimum elongation Lo = Lo = 80 mm (%) | 16 | 17 | 18 | |||
| Temperature | -20 | 0 | ||||
| Notch impact test. Min. absorbed energy | 27 | 27 | ||||
About Us
Gnee Steel Group, established in 2008, is a steel manufacturing company specialized in weathering steel materials and fabricated components.
With a full range of standard Corten steel grades (ASTM, EN, JIS, GB), we also offer custom processing services including cutting, welding, surface rusting, and large-scale project fabrication.
If you're looking for reliable weathering steel solutions or want to learn more about its applications, feel free to reach out at corten@gneesteelgroup.com - our team will respond promptly with professional support.
Contact now to get S355J0W Quote