What is equivalent to S355K2W Low-alloy High-strength Steel Plate

Sep 02, 2025 Leave a message

Products Description

 

S355K2W Low-alloy High-strength Steel Plate  is a kind of improved atmospheric corrosion resistance steel. S355K2W material Number is 1.8967. S355K2W steel plate V shaped impact test temperature is at -20 degree and min energy is 27J.Improved atmospheric corrosion resistance steel means weathering steel or atmosphere corrosion resistance steel.

S355K2W steel plate

S355K2W weathering steel sheet,"S" means S355K2W grade could be used in structural steel projects, 355 is the min yield strength. J0, J2 and K2 standard for the impact degree and energy in -20 temperature.W" means that the mainly different in their carbon and phosphorus contents and availability.

 

Specification

 

Product Name EN10025-5 S355K2W steel plate
Standard GB,ASTM/ASME,JIS,EN,DIN,BS,ISO
Material EN10025-5 S355K2W
Width 1000mm,1219mm,1250mm,1500mm,1800mm,2000mm,2200mm,2500mm,3000mm or as required
Thickness 0.4mm-280mm as customer's requirement
Length 2000mm,2438mm,3000mm,6000mm,as customer's requirement
Delivery States Hot-rolled, Controlled rolling, Normalizing, Annealing, Tempering, Quenching, N+T, Q+T,or as required MOQ: 500KG, We can accept sample order.

 

S355K2W chemical composition %

 

C

Si

Mn

Cu

P

S

Cr

N

0.19

0.55

0.45-1.60

0.20-0.60

0.035

0.035

0.35-0.85

0.010

 

S355K2W mechanical properties:

 

S355K2W Yield Strength

(Min Mpa)

S355K2W Tensile Strength

( Mpa)

S355K2W Impacting Test

t≤16

16<t≤40

40<t≤100

100<t

t≤100

100<t

℃

J

355

345

335

295

470-630

450-600

-20

40

*S355K2W heat treatment: Hot rolled, Control rolled, normalized, quenched and tempered, cold rolled.

 

Equivalent Grades of S355K2W Weathering Steel

 

Standard / Region Equivalent Grade / Designation
EN (Europe) S355K2W (+N)
ASTM / AASHTO (USA) A709 Grade 50W (bridge steel)
DIN / WBL 087 (Germany) E36WB4
AFNOR NFA 35-502 (France) -
BS 4360 (UK) -
JIS G3114 (Japan) -

 

EN10025-2 S355K2W Low-alloy High-strength Steel Plate Application

 

EN10025-2 S355K2W Steel Plate are used in Construction of Bridges, Highway Construction and Other Engineering construction

Corten Application

 

Other Terms

Packaging Details: Standard export seaworthy packing or as required.
 

Delivery Time: 30-50 days, 7 days for stock goods.
 

Loading Port: Shanghai ,Tianjin, Qingdao.
 

Offer Ability: 5 000MT/Per Month.
 

MOQ: 1 Pcs.

 

Contact now to get S355K2W Quote

 