What is High Strength WTSt 37-3 weathering steel plate

Sep 05, 2025 Leave a message

WTSt 37-3 Steel Description

 

WTSt 37-3 steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.

WTSt 37-3 Steel

WTSt 37-3 steel is the Equivalent grades as S235J2W ( 1.8961 ) steel in EN 10025 - 5 : 2004 standard and E24W4 steel in NFA 35-502 standard and also Fe360DK1 steel in UNI standard.
 

WTSt 37-3 Steel Delivery state

 

Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.

 

WTSt 37-3 steel application

 

Because of its low carbon content and fine-grained structure, WTSt 37-3 Steels with improved atmospheric corrosion resistance have excellent weldability.So WTSt 37-3 steel is mainly used for manufacturing welded,riveted or bolted structures.

corten

Moreover, WTSt 37-3 steel with improved atmospheric corrosion resistance has a wide range of applications: architecture, smokestacks, fabrication,freight wagons, silos, pylons and bridges.

 

WTSt 37-3 steel chemical composition by [%]

 

C % Mn % Cr % Si % CEV % S %
Max 0.13 0.2-0.6 0.4-0.8 Max 0.4 Max 0.44 Max 0.3
Cu % P %        
0.25-0.55 Max 0.035        


For long products the P and S content can be 0.005% higher
The WTSt 37-3 steels may show a Ni content of max. 0,65 %
The WTSt 37-3 steels shall contain at least one of the following elements: Al total ≥ 0,020 %, Nb: 0,015 - 0,060 %, V: 0,02 - 0,12 %, Ti: 0,02 - 0,10 %. If these elements are used in combination, at least one of them shall be present with the minimum content indicated.

 

WTSt 37-3 steel Mechanical properties

 

Grade Min. Yield Strength Mpa Tensile Strength MPa Impact
WTSt 37-3 Nominal Thickness (mm) Nominal Thickness (mm) degree J
Thick mm ≤16 >16
≤40
>40
≤63
>63
≤80
>80
≤100
>100
≤150
≤3 >3 ≤100 >100 ≤150 -20 27
WTSt 37-3 235 225 215 215 215 195 360-510 360-510 350-500

The tensile test values given in the table apply to longitudinal samples; in case of strip and sheet steel of widths of ≥600 mm they apply to transverse samples.


If WTSt 37-3 mechanical properties have been significantly modified by heavy coldforming, either stress relief annealing or normalised may be applied. Normalised should also be applied following hotforming outside of the temperature range of 750 - 1.050 °C and after overheating.

 

About us

 

One-Stop Weathering Steel Solutions for Diverse Project Needs
At Gnee, we provide full-process corten steel solutions including design, fabrication, surface treatment, and global shipping. Whether you're building a facade, a garden structure, or an industrial component, we deliver with speed, quality, and flexibility.

 

Our service highlights:

 

  • Drawing optimization and custom design
  • Precision fabrication with strict quality control
  • Various surface finishes: pre-rusted, painted, or anti-corrosion
  • Export-grade packaging and reliable worldwide logistics
  • Full technical support before and after sales

 

One supplier for everything – streamlined and efficient project delivery.

Contact now

 

gnee corten