Hot Rolled S355J0WP Plate: EN 10029 Tolerances and Uses

Oct 27, 2025 Leave a message

The Hot Rolling Route for Weathering Plate

Hot rolled S355J0WP plate starts as a continuously cast slab, which is reheated, rolled on a reversing or Steckel mill to the ordered thickness and then hot levelled and cut to length. Because the copper and chromium additions that give the grade its corrosion resistance also affect recrystallisation, plate mills control the finishing temperature and the cooling pattern carefully to obtain a uniform ferrite grain size from surface to centre. Thick plate is often rolled with a controlled reduction schedule, and where a higher strength and toughness balance is wanted, the plate is supplied in the normalised or thermo-mechanically rolled condition instead of as-rolled.

Hot rolling is the practical route for the heavier end of the weathering product range. Sections below about 6 mm are more usually supplied as coil from a hot strip mill, while plate from 6 mm upward is delivered flat with as-rolled or trimmed edges. Widths from 1500 mm to 4050 mm and lengths from 3000 mm to 15000 mm are standard, with cut-to-length programmes available for fabricated components.

Grade Data Applied to Plate Product

S355J0WP is defined in EN 10025-5, the part of the European structural steel series covering grades with improved atmospheric corrosion resistance, and it is the phosphorus-bearing variant of the S355 weathering family. Phosphorus is present at 0.06 to 0.15 percent, carbon is limited to 0.12 percent, manganese to 1.00 percent, silicon to 0.75 percent, and chromium and copper are added in the ranges 0.30 to 1.25 percent and 0.25 to 0.55 percent respectively.

Property Value for plate product
Minimum yield strength 355 MPa up to 16 mm, reducing to 335 MPa above 40 mm up to 63 mm
Tensile strength 470 to 630 MPa for thickness above 3 mm up to 100 mm
Minimum elongation 20 percent at the lower thicknesses
Impact requirement 27 J minimum Charpy V-notch at 0 degrees Celsius
Delivery conditions As-rolled, normalised or thermo-mechanically rolled

Because phosphorus raises the ductile to brittle transition temperature, plate in this grade is normally ordered in thicknesses where the material is bolted, riveted or lightly welded rather than heavily fabricated, and a J2 grade is selected when low-temperature toughness is required.

Dimensional Tolerances and Edge Condition

Dimensional requirements for hot rolled plate are ordered to EN 10029, which defines permissible deviations in thickness, width and length together with limits for flatness and edge camber. Thickness tolerances are the ones that most often determine whether a plate can be used without extra machining, so the tolerance class and the point of measurement should be agreed explicitly. Edge condition is ordered either as-rolled, where the natural rolled edge is retained, or as trimmed, where the edges are sheared or gas cut to a straight, square profile. Plate that will be profiled by the customer is usually ordered with trimmed edges and a defined squareness, and plate that will be welded on automatic lines is specified with a maximum camber so that fit-up is predictable.

Surface, Testing and Documentation

Surface condition is agreed against the EN 10163 series, which grades the permitted amount of surface imperfection, and plates for visible use are typically ordered to the more demanding classes. Thickness and internal soundness can be verified by ultrasonic examination to EN 10160 where the plate will carry primary loads or be used in pressure-retaining components. Delivery documentation includes an inspection certificate to EN 10204 3.1 with chemical analysis, tensile and elongation results, impact values at 0 degrees Celsius, heat number traceability and the declared delivery condition.

Where Hot Rolled S355J0WP Plate Is Used

Typical applications include flue gas ducts and air preheater casings, boiler casings and structural supports in power and process plant, architectural facades and cladding support systems, freight wagon panels and underframes, container frames, exhaust and ventilation components, and general outdoor structures that will be left unpainted. In each case the design must allow the surface to dry, and connections should avoid crevices and trapped moisture, since the protective layer only forms where the plate goes through wet and dry cycles. Where the environment is permanently wet, buried or chloride-rich, a coating system should be specified in addition to the weathering grade.

Frequently Asked Questions

Q: What thickness range is available in hot rolled S355J0WP?

A: Plate is commonly supplied from about 6 mm to 200 mm, although the yield strength table of the grade is normally published up to 63 mm, which is the practical range for this phosphorus-bearing steel.

Q: Which tolerance standard applies to the plate?

A: EN 10029 covers thickness, width, length, flatness and edge camber for hot rolled plate, and the required tolerance class should be stated in the order.

Q: Is the plate supplied with rolled or trimmed edges?

A: Both. Rolled edges are supplied where the natural profile is acceptable, and trimmed edges where straightness, squareness and a defined width are needed for fabrication.

Q: Can hot rolled S355J0WP be normalised?

A: Yes, normalised supply is available on request, and the delivery condition should be fixed when ordering because it affects properties, price and lead time.

Q: What testing can be ordered with the plate?

A: Ultrasonic examination to EN 10160 for internal soundness, plus the standard chemical, tensile and impact testing recorded on an inspection certificate to EN 10204 3.1.

Q: Is this grade suitable for boiler and flue gas equipment?

A: It is used for flue gas ducts, casings and supports, where the surface experiences wet and dry cycles. For acid dew point corrosion at the cold end of a gas path, a steel designed specifically for that service is the better choice.