What is the difference between Q345NH and Q390NH weathering steel?

Jan 12, 2026 Leave a message

Q345NH and Q390NH are both Chinese standard (GB/T 4171) low-alloy weathering steels, with the core difference lying in mechanical strength (yield/tensile strength), followed by minor variations in chemical composition, performance trade-offs, and application scenarios-both retain the signature corrosion resistance of weathering steel via Cu/Cr/P alloying.

info-230-223

1. Core Mechanical Property Differences (Key Distinction)

 
Compliant with GB/T 4171, the strength grade is the defining factor (the numbers 345/390 represent the minimum yield strength in MPa for plates ≤16mm thick):
 
Property Q345NH Q390NH
Minimum Yield Strength ≥345 MPa ≥390 MPa (13% higher than Q345NH)
Tensile Strength Range 470–630 MPa 510–660 MPa
Elongation (≥, t≤16mm) ≥21% ≥19% (slightly lower ductility)
Impact Toughness (0°C) ≥34 J (Charpy V-notch) ≥34 J (same toughness requirement)

info-565-551

2. Chemical Composition Variations (Driving Strength Differences)

 
Both contain the basic weathering alloy elements (Cu: 0.20–0.50%, Cr: 0.30–1.20%, P: 0.07–0.15%), but Q390NH has slightly adjusted alloying to boost strength:
 

Manganese (Mn): Q390NH has a higher Mn range (1.40–1.80%) vs. Q345NH (1.20–1.60%)-Mn enhances solid solution strengthening and grain refinement to raise yield strength.

Silicon (Si): Q390NH may have a marginally higher Si content (≤0.60%) vs. Q345NH (≤0.55%)-Si complements Mn in solid solution strengthening.

Weathering elements (Cu/Cr/P): Identical ranges for both grades, ensuring equivalent corrosion resistance (both form a stable patina in outdoor environments).

info-224-220

3. Performance Trade-Offs

 

Q345NH: Balances moderate strength and better ductility/ formability-easier to cold bend, weld, and fabricate into complex shapes without cracking.

Q390NH: Higher yield strength for heavier structural loads, but with slightly reduced ductility-requires more careful fabrication (e.g., larger bend radii, lower heat input during welding) to avoid residual stress or cracking.

Corrosion resistance: No difference-both grades achieve the same atmospheric corrosion resistance (Grade C per GB/T 4171) for outdoor use.

info-230-221

4. Typical Application Scenarios

 
The strength difference dictates their use cases, with both suited for outdoor, corrosion-prone environments:
 

Q345NH: General weathering steel structures with moderate loads-e.g., building facades, garden pergolas, low-rise structural frames, guardrails, small-diameter pipes, and decorative components.

Q390NH: High-strength weathering steel structures with heavy loads-e.g., high-rise building support beams, bridge components, large-span pergolas, wind turbine towers, and heavy-duty transport equipment frames.