Which steel materials equivalent to A709 GR 50 Weathering Steel Sheet?

Dec 04, 2025 Leave a message

ASTM A709 Grade 50 is one of the most commonly used structural steel grades for bridge construction under the ASTM A709/A709M specification.

 

This standard includes multiple strength levels-A709 Gr 36, Gr 50, Gr 50S, Gr 50W, HPS 50W, HPS 70W, and HPS 100W-designed to meet different performance and environmental requirements for modern bridge engineering.

 

ASTM A709 Grade 50

 

For users working with international projects or needing a comparable Chinese alternative, Q345qC, specified under GB/T 714, is widely recognised as the closest equivalent material to ASTM A709 Gr 50.

 

Both steels are designed for bridge-building applications, provide good weldability, and offer reliable structural strength. Q345qC also demonstrates a certain level of atmospheric corrosion resistance when left unpainted, making it suitable for outdoor structures.

 

Gnee Steel Plate supplies 4 ft and 8 ft wide A709 Gr 50 bridge steel plates from stock in our port warehouse, ready for shipment within 3 days.

 

A709 Gr 50 vs Q345qC Comparison

 

 

Chemical Composition (Heat Analysis, Max %)

StandardGradeCMnPSSiCrNiCuN
ASTM A709/A709MA709 Gr 500.231.350.0400.0500.40----
GB/T 714Q345qC0.180.9–1.60.0300.0250.550.300.300.300.008

Analysis:

Q345qC is generally lower in carbon, meaning better weldability.

Q345qC includes alloying elements (Cr, Ni, Cu) that enhance corrosion resistance compared to A709 Gr 50.

Si content is slightly higher in Q345qC, helping improve strength.

 

Mechanical Properties

StandardGradeThicknessYield Strength (MPa)Tensile Strength (MPa)
ASTM A709/A709MA709 Gr 50T ≤ 40 mm345 min.450 min.
GB/T 714Q345qCT ≤ 50 mm345 min.490 min.

Both grades deliver the same minimum yield strength (345 MPa).

 

Q345qC offers a higher minimum tensile strength (490 MPa) compared to A709 Gr 50 (450 MPa).

Q345qC allows thicker material (up to 50 mm) with the same mechanical performance.

 

Products Applications

 

 

Both A709 Gr 50 and Q345qC are widely used in:

Highway bridges

Railway bridges

Long-span steel structures

Box girders & beam structures

Trusses and arch bridges

Structural components requiring high strength and low alloy properties

 

Q345qC, like A709 Gr 50, is engineered to perform reliably under dynamic loads, temperature variations, and outdoor atmospheric conditions.

 

Why Q345qC is the Best Equivalent to A709 Gr 50

 

 

Matching CriteriaComparison Result
Strength Level✔ Equivalent
Yield Strength✔ Same (345 MPa)
Tensile Strength✔ Q345qC is higher
Weldability✔ Q345qC better (lower carbon)
Atmospheric Resistance✔ Q345qC slightly better (Cu, Ni, Cr added)
Bridge Application Suitability✔ Fully equivalent


Q345qC is the closest and most practical Chinese equivalent to ASTM A709 Grade 50, offering comparable strength, enhanced corrosion resistance, and excellent weldability.

 

Contact now

 

info-363-670

 

What is A709 grade 50W steel?

ASTM A709-50W is a standard specification for structural steel primarily in the fabrication of steel bridges. ASTM A709-50W covers high strength, low allow steel structural shapes, plates and bars.

 

What is ASTM A709 steel grade?

The ASTM A709 is the Standard Specification for Structural Steel for Bridges and encompasses carbon, high-strength low-alloy, and quenched and tempered alloy steels used as structural plates in the construction of bridges. SSAB offers the following five grades of A709; 36, 50, 50W, HPS 50W and HPS 70W.

 

What is the difference between ASTM A572 Grade 50 and ASTM A709 Grade 50?

A572 Grade 50: Used in a wide range of structural applications, including buildings, transmission towers, equipment, and general construction. It's not specifically optimized for bridges. A709 Grade 50: Primarily used for bridge construction and other structures where enhanced toughness and weldability are critical.

 

What is the yield strength of ASTM A709 grade 50?

Grade 50 steel of this specification requires a minimum yield strength of 50 ksi. Used as structural members in bridge building or for similar structures.

 

What is the difference between ASTM A36 and A709?

ASTM A709 grade 36 is a bridge material wherein carbon adds to the strength and hardenability of the steel. A36 has less than0. 30% carbon and thus, do not possess high hardenability. ASTM A709 grade 36 steel plate has improved corrosion resistance and can be used in outdoor applications.

 

What is ASTM A572 grade 50 equivalent to?

ASTM A572 Grade 50 is equivalent to several other steel grades, with the most common international equivalents being S355JR (European standard) and Q345B (Chinese standard). The best equivalent depends on the specific project requirements, so it is always best to consult material specifications and a specialist to confirm compatibility.

 

What is the difference between ASTM A36 and ASTM A572 GR 50?

As mentioned earlier, A36 is steel that has a minimum yield strength of 36,000 PSI. This grade derives its strength from a combination of carbon and manganese. On the other hand, A572-50, for example, is a type of steel with a minimum yield strength of 50,000 PSI.

 

What is the difference between A572 and s355?

In summary, both ASTM A572 Grade 50 and S355JR are excellent choices for structural steel applications, with ASTM A572 Grade 50 providing higher strength capabilities and S355JR offering versatility and widespread use in European construction projects.

 

Is A572 steel corrosion resistant?

A572 steel is typically used in structural applications due to its high strength, ductility, weldability and corrosion resistance. These applications include structural sections, reinforcing bars, bridges, skyscrapers and houses.

 

Grades Of Carbon and Low-alloy High-strength Steels Supplied By GNEE
ASTM/ASMEASTM A36/A36MASTM A36   
ASTM A283/A283MASTM A283 Grade AASTM A283 Grade BASTM A283 Grade CASTM A283 Grade D
ASTM A514/A514MASTM A514 Grade AASTM A514 Grade BASTM A514 Grade CASTM A514 Grade E
ASTM A514 Grade FASTM A514 Grade HASTM A514 Grade JASTM A514 Grade K
ASTM A514 Grade MASTM A514 Grade PASTM A514 Grade QASTM A514 Grade R
ASTM A514 Grade SASTM A514 Grade T  
ASTM A572/A572MASTM A572 Grade 42ASTM A572 Grade 50ASTM A572 Grade 55ASTM A572 Grade 60
ASTM A572 Grade 65   
ASTM A573/A573MASTM A573 Grade 58ASTM A573 Grade 65ASTM A573 Grade 70 
ASTM A588/A588MASTM A588 Grade AASTM A588 Grade BASTM A588 Grade CASTM A588 Grade K
ASTM A633/A633MASTM A633 Grade AASTM A633 Grade CASTM A633 Grade DASTM A633 Grade E
ASTM A656/A656MASTM A656 Grade 50ASTM A656 Grade 60ASTM A656 Grade 70ASTM A656 Grade 80
ASTM A709/A709MASTM A709 Grade 36ASTM A709 Grade 50ASTM A709 Grade 50SASTM A709 Grade 50W
ASTM A709 Grade HPS 50WASTM A709 Grade HPS 70WASTM A709 Grade 100ASTM A709 Grade 100W
ASTM A709 Grade HPS 100W   
ASME SA36/SA36MASME SA36   
ASME SA283/SA283MASME SA283 Grade AASME SA283 Grade BASME SA283 Grade CASME SA283 Grade D
ASME SA514/SA514MASME SA514 Grade AASME SA514 Grade BASME SA514 Grade CASME SA514 Grade E
ASME SA514 Grade FASME SA514 Grade HASME SA514 Grade JASME SA514 Grade K
ASME SA514 Grade MASME SA514 Grade PASME SA514 Grade QASME SA514 Grade R
ASME SA514 Grade SASME SA514 Grade T  
ASME SA572/SA572MASME SA572 Grade 42ASME SA572 Grade 50ASME SA572 Grade 55ASME SA572 Grade 60
ASME SA572 Grade 65   
ASME SA573/SA573MASME SA573 Grade 58ASME SA573 Grade 65ASME SA573 Grade 70 
ASME SA588/SA588MASME SA588 Grade AASME SA588 Grade BASME SA588 Grade CASME SA588 Grade K
ASME SA633/SA633MASME SA633 Grade AASME SA633 Grade CASME SA633 Grade DASME SA633 Grade E
ASME SA656/SA656MASME SA656 Grade 50ASME SA656 Grade 60ASME SA656 Grade 70ASME SA656 Grade 80
ASME SA709/SA709MASME SA709 Grade 36ASME SA709 Grade 50ASME SA709 Grade 50SASME SA709 Grade 50W
ASME SA709 Grade HPS 50WASME SA709 Grade HPS 70WASME SA709 Grade 100ASME SA709 Grade 100W
ASME SA709 Grade HPS 100W   
EN10025EN10025-2EN10025-2 S235J0EN10025-2 S275J0EN10025-2 S355J0EN10025-2 S355K2
EN10025-2 S235JREN10025-2 S275JREN10025-2 S355JREN10025-2 S420J0
EN10025-2 S235J2EN10025-2 S275J2EN10025-2 S355J2 
EN10025-3EN10025-3 S275NEN10025-3 S355NEN10025-3 S420NEN10025-3 S460N
EN10025-3 S275NLEN10025-3 S355NLEN10025-3 S420NLEN10025-3 S460NL
EN10025-4EN10025-4 S275MEN10025-4 S355MEN10025-4 S420MEN10025-4 S460M
EN10025-4 S275MLEN10025-4 S355MLEN10025-4 S420MLEN10025-4 S460ML
EN10025-6EN10025-6 S460QEN10025-6 S460QLEN10025-6 S460QL1EN10025-6 S500Q
EN10025-6 S500QLEN10025-6 S500QL1EN10025-6 S550QEN10025-6 S550QL
EN10025-6 S550QL1EN10025-6 S620QEN10025-6 S620QLEN10025-6 S620QL1
EN10025-6 S690QEN10025-6 S690QLEN10025-6 S690Q1EN10025-6 S890Q
EN10025-6 S890QLEN10025-6 S890QL1EN10025-6 S960QEN10025-6 S960QL
JISJIS G3101JIS G3101 SS330JIS G3101 SS400JIS G3101 SS490JIS G3101 SS540
JIS G3106JIS G3106 SM400AJIS G3106 SM400BJIS G3106 SM400CJIS G3106 SM490A
JIS G3106 SM490YAJIS G3106 SM490BJIS G3106 SM490YBJIS G3106 SM490C
JIS G3106 SM520BJIS G3106 SM520CJIS G3106 SM570 
DINDIN 17100DIN17100 St52-3DIN17100 St37-2DIN17100 St37-3DIN17100 RSt37-2
DIN17100 USt37-2   
DIN 17102DIN17102 StE315DIN17102 EStE315DIN17102 TStE315DIN17102 WStE315
DIN17102 StE355DIN17102 EStE355DIN17102 TStE355DIN17102 WStE355
DIN17102 StE380DIN17102 EStE380DIN17102 TStE380DIN17102 WStE380
DIN17102 StE420DIN17102 EStE420DIN17102 TStE420DIN17102 WStE420
DIN17102 StE460DIN17102 EStE460DIN17102 TStE460DIN17102 WStE460
DIN17102 StE500DIN17102 EStE500DIN17102 TStE500DIN17102 WStE500
DIN17102 EStE285   
GBGB/T700GB/T700 Q235AGB/T700 Q235BGB/T700 Q235CGB/T700 Q235D
GB/T700 Q275   
GB/T1591GB/T1591 Q345AGB/T1591 Q390AGB/T1591 Q420AGB/T1591 Q420E
GB/T1591 Q345BGB/T1591 Q390BGB/T1591 Q420BGB/T1591 Q460C
GB/T1591 Q345CGB/T1591 Q390CGB/T1591 Q420CGB/T1591 Q460D
GB/T1591 Q345DGB/T1591 Q390DGB/T1591 Q420DGB/T1591 Q460E
GB/T1591 Q345EGB/T1591 Q390E  
GB/T16270GB/T16270 Q550CGB/T16270 Q550DGB/T16270 Q550EGB/T16270 Q550F
GB/T16270 Q620CGB/T16270 Q620DGB/T16270 Q620EGB/T16270 Q620F
GB/T16270 Q690CGB/T16270 Q690DGB/T16270 Q690EGB/T16270 Q690F
GB/T16270 Q800CGB/T16270 Q800DGB/T16270 Q800EGB/T16270 Q800F
GB/T16270 Q890CGB/T16270 Q890DGB/T16270 Q890EGB/T16270 Q890F
GB/T16270 Q960CGB/T16270 Q960DGB/T16270 Q960EGB/T16270 Q960F
GB/T16270 Q500