Products Description
09CrCuSb Steel tubing is a low alloy structural steel.Compared with other types of steel such as mild steel, Corten, CR1A, ND steel has excellent corrosion resistance and mechanical properties.
Because the ND steel can form the fine and close passive film that several times of matrixes are rich in elements such as Cr, Cu, Sb, Ti that is higher than of one deck densification on its surface in corrosion process, thereby has the ability of high sulfuric-resisting dew point corrosion.
Test shows that in 70 ℃ of 50% aqueous sulfuric acid, the ability of the anti-uniform corrosion of ND steel of the present invention is 10 times of 20g soft steel, is 304 stainless 3 times, is 1.5 times of Japanese similar steel grade CR1A
09CrCuSb (ND steel) steel pipe tube used in power plants and refineries to manufacture economizers, air preheaters, heat exchangers and evaporators that work in high-sulfur flue gas to protect against sulfur-containing flue gas condensation.
09CrCuSb Chemical Composition
|
Grade |
Composition(%) |
|||||||
|
C |
Si |
Mn |
Cr |
Cu |
Sb |
P |
S |
|
|
09CrCusb |
≤0.10 |
0.20-0.40 |
0.35-0.65 |
0.70-1.20 |
0.25-0.45 |
≤0.10 |
≤0.10 |
≤0. |
09CrCuSb Mechanical Properties
|
Grade |
Tensile strength(Mpa) |
Yield strength(Mpa) |
Percentage elongation(A %) |
|
09CrCuSb |
390-550 |
≥245 |
≥25 |
09CrCuSb tube Applications
The outstanding corrosion resistance of 09CrCuSb (ND) steel makes it an essential material for industries operating in severe service environments.
In power generation plants, ND steel pipes are widely applied in the manufacture of economizers, air preheaters, and heat exchangers, where protection against sulfur-containing flue gases is critical.
In the chemical and petrochemical industries, ND steel is used to build piping systems, reactors, and heat exchangers that must withstand aggressive and corrosive media.
Additionally, the marine and offshore sectors benefit from its exceptional durability, employing it in the fabrication of components exposed to seawater and other harsh conditions.