Q460NH steel plate,under China GB/T 4171 standard, Q460NH steel plate is a kind of weathering steel. Q460NH steel plate is widely used to: container, chimney, railway construction and other outdoor steel such as a large outdoor sculpture steel.

 

Q460NH steel plate

 

Q460NH steel plate Specification

 

Thickness:3mm-40mm,as customer's requirement

Width:1500mm-3000mm,as customer's requirement

Length:4000mm-13000mm,as customer's requirement

 

Q460NH steel plate Chemical composition(%)

 

C

Si

Mn

P

S

Cu

Ni

Cr

0.12

0.65

1.50

0.025

0.030

0.20-0.55

0.12-0.65

0.30-1.25

 

 

Q460NH steel plate Mechanical properties

 

Thickness (mm)

Q460NH

≤ 16

> 16 ≤ 40

> 40 ≤ 60

>60

Yield strength (≥Mpa)

460

450

440

440

Tensile strength (Mpa)

570-730

 

Applications of China GB/T 4171 Q460NH Weather Resistant Steel Plate

 

Q460NH Weather Resistant Steel Plate are extensive, suitable for outdoor structures that require high strength and long-term atmospheric corrosion resistance..

 

In the transportation sector, it is commonly used for vehicle underframes, railway wagon bodies, and bridge load-bearing components, with typical mechanical properties including a yield strength of approximately 460 MPa, tensile strength of 570–690 MPa, and elongation of 18–22%, maintaining excellent toughness and reliability even in low-temperature or humid environments.

 

In construction projects, Q460NH steel plates are applied to bridge main beams, tower supports, large building frameworks, and decorative cladding.

 

The surface naturally forms a dense oxide layer approximately 50–100 μm thick, which effectively slows further corrosion, providing a service life of 20–30 years in urban or industrial environments and over 25 years in coastal or high-humidity conditions.

 

Additionally, Q460NH steel plates are widely used in container manufacturing, shipbuilding, and large outdoor facilities. Thanks to their high strength, corrosion resistance, and low maintenance requirements, they are a reliable choice of weathering steel for engineering and construction applications.

 