Products Description
09CrCuSb (ND) High-Performance Corrosion-Resistant Seamless Tubes are widely used in the manufacture of economizers, air preheaters, heat exchangers and evaporators that are used in 100-high sulfur-containing flue gas, to resist dew point corrosion of sulfur-containing flue gas.

ND (09CrCuSb) steel tube also has the ability to resist chloride ion corrosion. The main reference standard of ND steel pipe is internal standard (soaked in 50% H2SO4 solution at 70 degrees Celsius for 24 hours).
Compared with other steels such as low carbon steel, corten and cr1a, ND steel has excellent corrosion resistance and mechanical properties.
09CrCuSb tube Specification
| Specification | Specification |
| 19*2-4mm | 76-114 * 4-10mm |
| 25 * 2-4mm | 133-140 * 6-14mm |
| 32 * 2-5mm | 159-219 * 21-35mm |
| 38-42 * 3-5mm | 273-325 * 7-50mm |
| 51-63 * 3-5mm | 356-630 * 10-20mm |
Chemical Composition of 09CrCuSb (ND Steel) Seamless Pipe
| Element | Content (%) |
|---|---|
| Carbon (C) | 0.06 – 0.12 |
| Silicon (Si) | 0.25 – 0.75 |
| Manganese (Mn) | 0.50 – 1.25 |
| Phosphorus (P) | ≤ 0.020 |
| Sulfur (S) | ≤ 0.020 |
| Chromium (Cr) | 0.30 – 1.25 |
| Copper (Cu) | 0.25 – 0.55 |
| Antimony (Sb) | 0.010 – 0.040 |
Mechanical Properties of 09CrCuSb (ND Steel) Seamless Pipe
| Property | Value | Unit / Note |
|---|---|---|
| Tensile Strength | ≥ 450 | MPa |
| Yield Strength | ≥ 315 | MPa |
| Elongation | ≥ 22 | % |
| Impact Toughness | ≥ 34 | J/cm² |
Products Photos


Products Application
The versatility of Corten seamless steel pipes makes them ideal for various applications, including:
- Structural components in buildings and bridges.
- Piping systems for industrial and infrastructure projects.
- Decorative elements in outdoor sculptures and landscaping.