What is ASTM A847 Gr.1 Cold Formed Welded Pipe?

ASTM A847 is the standard specification for cold-formed welded and seamless high-strength, low-alloy (HSLA) structural tubing with improved atmospheric corrosion resistance.

 

ASTM A847 cold formed welded pipe is designed for structural applications requiring a combination of mechanical strength, atmospheric corrosion resistance and fabrication flexibility. It is available in round, square, rectangular and special-shaped sections for bridges, buildings, walkways, railings and other outdoor structures.

 

As a professional steel supplier, Gnee provides ASTM A847 weathering steel tubes in different dimensions, wall thicknesses and lengths. Our ASTM A847 cold formed welded pipe combines a minimum yield strength of 345 MPa, a minimum tensile strength of 483 MPa and a minimum elongation of 19%.

 

When properly exposed to suitable atmospheric conditions, the steel develops a protective oxide layer that can reduce the need for conventional painting and repeated coating maintenance.

ASTM A847 Gr.1 Cold Formed Welded Pipe
A847 Gr.1 Cold Formed Welded Pipe

Scope & Applicable Standards

ASTM A847 covers structural tubing used in welded, riveted and bolted construction. The specification includes cold-formed welded and seamless tubing, with round, square, rectangular and special-shaped sections.

Item

Detail

Standard

ASTM A847/A847M

Material Type

High-Strength Low-Alloy Weathering Steel

Manufacturing Process

Cold-Formed Welded

Welded Maximum Periphery

88 in. (2,235 mm)

Welded Maximum Wall Thickness

1.000 in. (25.4 mm)

Seamless Maximum Periphery

32 in. (813 mm)

Seamless Maximum Wall Thickness

0.500 in. (12.7 mm)

 

ASTM A847 Gr.1 Cold Formed Welded Pipe Chemical Composition

The chemical composition of ASTM A847 weathering steel is controlled to provide the required strength and atmospheric corrosion resistance.

Element

Chemical Composition (%)

Carbon (C)

0.20 max

Manganese (Mn)

1.35 max

Phosphorus (P)

0.15 max

Sulfur (S)

0.05 max

Copper (Cu)

0.20 min

 

Mechanical Properties of ASTM A847 Gr.1 Steel Tube

The mechanical properties of ASTM A847 cold formed welded pipe make it suitable for structural components subjected to tensile forces and external loads. The minimum yield strength is 50 ksi, while the minimum tensile strength is 70 ksi.

 

Mechanical Property

Minimum Requirement

Yield Strength

345 MPa (50 ksi)

Tensile Strength

483 MPa (70 ksi)

Elongation in 2 in. (50 mm)

19%

Yield-to-Tensile Strength Ratio

≤ 71.43%*

 

Mechanical Performance Comparison

Parameter

ASTM A847

Reference Value of ASTM A423 Gr.1

Yield Strength (MPa)

345

240

Tensile Strength (MPa)

483

415

Yield Strength Difference

+43.75%

Baseline

Tensile Strength Difference

+16.39%

Baseline

 

What are the Advantages of ASTM A847 Corten Square Steel Tube?

ASTM A847 Corten square steel tube combines structural strength with improved atmospheric corrosion resistance. Compared with conventional carbon steel structures that require protective coating systems, properly exposed A847 weathering steel can develop a stable oxide layer under suitable wet-dry atmospheric cycles.

1. Atmospheric Corrosion Resistance

ASTM A847 weathering steel contains copper and other controlled alloying elements that contribute to the formation of a protective oxide layer. The surface gradually develops a brown weathered appearance under suitable atmospheric conditions.

 

Unlike conventional painted structural steel, A847 steel square tubes can be used without an additional paint system in applications where the environment and structural design permit bare weathering steel.

2. Reduced Maintenance Costs

The natural weathering surface can eliminate the need for routine repainting in suitable applications. According to the commercial reference information supplied for this article, initial cost savings are estimated at 10%–15%, while lifecycle cost savings are stated to reach at least 30%.

 

These percentages are reference commercial estimates rather than universal ASTM performance guarantees. Actual savings depend on project design, coating specifications, labor costs, exposure conditions and maintenance intervals.

 

3. High Structural Strength

With a minimum yield strength of 345 MPa and minimum tensile strength of 483 MPa, ASTM A847 steel structural square tube can be used in load-bearing structural components. Engineers can evaluate section dimensions and wall thickness according to the design loads and applicable structural codes.

 

4. Fabrication Flexibility

Cold-formed welded steel tubes can be supplied in square and rectangular configurations. They can be processed through cutting, drilling, welding and other fabrication operations according to project requirements.

 

Manufacturing Process of Cold Formed Welded Steel Tube

The manufacturing process of ASTM A847 cold formed welded pipe involves several stages, from steel coil preparation to final inspection. Cold forming shapes the steel into the required cross-section, while welding joins the formed edges to produce a continuous structural tube.

 

Manufacturing Process

Production Stage

Raw Material Preparation

Uncoiling

Cold Forming

Welding

Sizing

Cutting

Inspection

Packaging

 

Cold Forming and Welding Process

During cold forming, steel strips pass through a series of forming rolls that gradually change the flat strip into the required tubular profile. For square steel structural tubes, the formed section is adjusted to achieve the specified corner geometry and outside dimensions.

 

The longitudinal edges are then joined by welding. After welding, the tube passes through sizing equipment to control its final dimensions. The finished cold-formed welded steel tube is cut to the required length and inspected before delivery.

 

Standard Sizes and Dimensions of ASTM A847 Square Steel Pipe

ASTM A847 structural tubing is available in different outside dimensions, wall thicknesses and section configurations. Square and rectangular steel tubes are commonly selected according to structural loads, connection designs and fabrication requirements.

 

The ASTM A847/A847M-21 specification provides maximum manufacturing limits for welded and seamless products. The following table presents these limits.

Parameter

Welded Tubing

Maximum Periphery

2,235 mm

Maximum Wall Thickness

25.4 mm

Section Shapes

Round / Square / Rectangular / Special

 

Available Product Dimensions

Product Parameter

Available Options

Shape

Square / Rectangular / Round

Outside Dimensions

Customized

Wall Thickness

Customized

Length

Fixed Length / Customized

Surface

Mill Finish / Natural Weathered Surface

Processing

Cutting / Drilling / Welding / Fabrication

For custom ASTM A847 cold formed square tube orders, please provide the outside dimensions, wall thickness, length, quantity and required delivery destination.

 

Gnee can evaluate the manufacturing specifications and provide a quotation according to your project requirements.

 

Atmospheric Corrosion Resistance of ASTM A847 Weathering Steel Tubes

Atmospheric corrosion resistance is one of the main reasons for selecting ASTM A847 Corten steel square tubes in outdoor structural projects.

 

When exposed to alternating wet and dry conditions, the alloying elements in weathering steel contribute to the development of a protective oxide layer. This layer gradually changes the surface from its initial orange-brown appearance to a darker brown patina.

 

Unlike ordinary carbon steel, which generally requires a protective coating to reduce atmospheric corrosion, ASTM A847 can be used unpainted in suitable environments.

 

However, weathering steel does not provide the same performance in every environment. Continuous moisture, water accumulation, marine salt exposure and sheltered areas without sufficient drying can interfere with protective patina formation.

 

Applications of ASTM A847 Steel Structural Square Tube

ASTM A847 steel structural square tube is used in structural engineering, infrastructure, transportation and architectural projects. Its combination of a minimum yield strength of 345 MPa and atmospheric corrosion resistance makes it suitable for evaluating in outdoor load-bearing structures.

1. Bridges and Walkways

ASTM A847 square and rectangular tubes can be used in bridge trusses, pedestrian bridge components, handrails, support frames and other structural members. Their section geometry provides flexibility for designing welded and bolted connections.

 

2. Building Structures

Cold formed welded steel tubes can be incorporated into building frameworks, roof supports, space frame structures and exterior architectural components. Square and rectangular sections are suitable for projects requiring defined structural profiles.

 

3. Railings and Guardrails

Corten square steel tubes can be fabricated into outdoor railings, pedestrian barriers and protective structures. Their natural weathered appearance can also be incorporated into architectural designs.

 

4. Utility and Lighting Poles

Weathering steel structural tubing can be considered for utility poles, lighting supports and other outdoor support structures, subject to the required structural design and environmental assessment.

 

5. Architectural and Landscape Projects

Corten steel square tubes can be used in landscape frameworks, outdoor shelters, decorative structures and architectural support systems. The developing brown patina provides a natural surface appearance without requiring conventional decorative paint.

 ASTM A847 Steel Structural Square Tube
A847 Weathering steel structural tubing
A847 Corten steel structural tubing

Welding, Testing and Inspection Requirements for ASTM A847 Tubes

ASTM A847 cold formed welded pipe is designed for structural fabrication involving welding, riveting and bolting. Welding procedures should be selected according to the steel composition, material thickness, joint configuration and intended service conditions.

 

For structural projects, inspection and documentation are important for verifying material quality and product traceability.

Inspection Item

Chemical Analysis

Tensile Test

Elongation Test

Dimensional Inspection

Weld Inspection

Visual Inspection

MTC

Third-Party Inspection

Cost-Benefit Analysis of ASTM A847 Corten Steel Square Tubes

ASTM A847 Corten steel square tubes can reduce coating-related expenses in suitable outdoor structural applications. Their natural weathering surface can eliminate the need for conventional painting when the exposure environment permits uncoated use.

According to the commercial reference information provided, the estimated financial benefits include:

Cost Factor

Reference Percentage

Initial Cost Savings

10%–15%

Lifecycle Cost Savings

At least 30%

Painting Requirement

Can be eliminated

Repainting Requirement

Can be eliminated

The actual cost difference depends on the initial material price, fabrication expenses, transportation, coating specifications and maintenance requirements.

 

ASTM A847 vs ASTM A500 Structural Steel Tubes

ASTM A847 and ASTM A500 are both used for structural steel tubing, but their main differences involve atmospheric corrosion resistance and material requirements.

 

ASTM A500 covers cold-formed welded and seamless carbon steel structural tubing, while ASTM A847 covers high-strength low-alloy structural tubing with improved atmospheric corrosion resistance.

Comparison Item

ASTM A847

ASTM A500 Grade C

Material Type

HSLA Weathering Steel

Carbon Steel

Manufacturing

Cold-Formed Welded / Seamless

Cold-Formed Welded / Seamless

Minimum Yield Strength

345 MPa

345 MPa

Minimum Tensile Strength

483 MPa

425 MPa

Minimum Elongation

19%

Depends on product dimensions

Atmospheric Corrosion Resistance

Improved

Conventional Carbon Steel

Protective Surface

Natural Weathering Patina

Usually Requires Protective Coating for Outdoor Exposure

 

Why Choose Gnee as Your ASTM A847 Cold Formed Welded Pipe Supplier?

Gnee supplies weathering steel products for structural and industrial applications. Our product range includes ASTM A847 cold formed welded pipe, Corten square steel tube, rectangular steel tubing and other weathering steel products.

 

We support customers with product selection, dimensional customization, material documentation and export order coordination.

Our Supply Services

Service

Details

Product Supply

ASTM A847 Weathering Steel Tubes

Section Shapes

Square / Rectangular / Round

Dimensions

Customized

Wall Thickness

Customized

Cutting

Available Upon Request

Packaging

Export Packaging

Quality Documents

MTC / Inspection Reports

Samples

Subject to Availability

Shipping

International Export

ASTM A847 Gr.1 Steel Tube
ASTM A847 Gr.1 cold formed welded pipe
A847 cold formed square tube

Contact Gnee For ASTM A847 Cold Formed Welded Pipe

 

Looking for an ASTM A847 cold formed welded pipe manufacturer or supplier?

 

Gnee provides ASTM A847 weathering steel tubing for bridges, buildings, structural frameworks and outdoor infrastructure projects. Whether you need Corten square steel tubes, cold formed square tube or rectangular steel structural tubing, our team can help evaluate your product requirements.