JIS G3125 SPA-H electric resistance welded pipe

Nov 26, 2026 Leave a message

JIS G3125 SPA-H Electric Resistance Welded Pipe

GNEE supplies JIS G3125 SPA-H electric resistance welded pipe manufactured from atmospheric corrosion-resistant SPA-H steel. These ERW steel pipes are produced by forming SPA-H steel strip or plate into a round section and joining the longitudinal seam through electric resistance welding.

 

The product is suitable for container manufacturing, railway structures, transportation equipment, steel structures and industrial applications requiring weathering steel.

 

SPA-H is a weathering steel grade specified in JIS G 3125. Its alloy composition includes copper (Cu), chromium (Cr), nickel (Ni) and phosphorus (P). Under suitable atmospheric exposure conditions, SPA-H steel can develop a protective rust layer that reduces the rate of further corrosion compared with ordinary carbon steel.

SPA-H welded steel pipes

 

GNEE provides SPA-H welded steel pipes according to confirmed dimensions, material requirements, manufacturing conditions and inspection specifications. Customers can request an ERW steel pipe quotation, technical data, available sizes and material certification before placing an order.

 

What Is JIS G3125 SPA-H Electric Resistance Welded Pipe?

JIS G3125 SPA-H electric resistance welded pipe is a weathering steel tube manufactured from SPA-H steel specified under JIS G 3125.

 

During ERW production, steel strip is formed into a cylindrical shape, and the longitudinal edges are heated by electrical resistance and pressed together to create a welded seam.

 

JIS G 3125 specifies the chemical composition and mechanical properties of atmospheric corrosion-resistant rolled steel. It is not a complete finished-pipe product standard covering every ERW pipe dimension, weld inspection requirement or pressure rating.

 

Finished SPA-H electric resistance welded pipe should therefore be supplied according to the agreed product specification, including the applicable material standard, dimensions, manufacturing process, testing and acceptance requirements.

 

SPA-H ERW Steel Pipe Manufacturing Process

SPA-H electric resistance welded tubing is manufactured through a series of forming and welding operations.

Raw Material Selection: SPA-H steel strip or plate is selected according to the agreed material specification and heat number.

Slitting and Cutting: The steel material is prepared to the required width for pipe forming.

Roll Forming: The steel strip is gradually formed into a round tubular section.

Electric Resistance Welding: The longitudinal edges are heated by electrical resistance and joined under pressure.

Weld Seam Finishing: The weld bead is trimmed or finished according to the agreed manufacturing requirements.

Sizing and Straightening: The welded tube is calibrated to the specified outside diameter and straightness.

Cutting to Length: The ERW steel pipe is cut to the ordered length.

Inspection and Marking: Finished pipes are checked against the purchase specification and marked for identification.

JIS G3125 SPA-H electric resistance welded pipe
SPA-H ERW Steel Pipe
SPA-H ERW Steel Pipe

The ERW process creates a longitudinal weld seam. It does not produce a seamless pipe. The weld seam position, surface condition, dimensional tolerance and inspection scope should be confirmed in the purchase order.

 

JIS G3125 SPA-H ERW Steel Pipe Specifications

Parameter Specification
Product Name SPA-H Electric Resistance Welded Pipe
Material Standard JIS G 3125
Product Type ERW Steel Pipe / Welded Steel Tube
Outside Diameter 21- 76 mm above 300mm
Wall Thickness 1.5- 4.0 mm
Pipe Length Fixed Length / Random Length / Custom Length, as agreed
Surface Condition As-welded / Descaled / Coated, as agreed
Material Documentation Mill Test Certificate (MTC), as agreed

Note: JIS G 3125 applies to the SPA-H steel material. Finished pipe dimensions, tolerances, weld acceptance criteria and additional testing must be specified separately or agreed between the purchaser and supplier.

 

Chemical Composition of JIS G3125 SPA-H Steel (%)

SPA-H weathering steel contains alloying elements that contribute to atmospheric corrosion resistance. The following chemical composition is based on the SPA-H data provided for this product page. The applicable JIS edition and actual heat analysis should be verified against the mill test certificate.

Element SPA-H (%)
Carbon (C) ≤ 0.12
Silicon (Si) 0.20–0.75
Manganese (Mn) ≤ 0.60
Phosphorus (P) 0.070–0.150
Sulfur (S) ≤ 0.035
Copper (Cu) 0.25–0.55
Chromium (Cr) 0.30–1.25
Nickel (Ni) ≤ 0.65

 

Mechanical Properties of SPA-H Steel

The following values refer to SPA-H steel material under JIS G 3125. They are not automatically the finished ERW pipe acceptance values. The mechanical properties of the completed SPA-H steel tube should be confirmed according to the agreed pipe specification and testing requirements.

Property Thickness Requirement
Yield Strength All applicable thicknesses ≥ 355 MPa
Tensile Strength All applicable thicknesses ≥ 490 MPa
Elongation ≤ 6.0 mm ≥ 22%
Elongation > 6.0 mm ≥ 15%

The finished pipe may be affected by forming, welding, sizing and any subsequent heat treatment. If the project requires tensile testing of the finished pipe or weld, the test location, specimen type, frequency and acceptance criteria should be agreed before production.

 

SPA-H Electric Resistance Welded Pipe Dimensions

The following outside diameters can be used as reference sizes for small-diameter SPA-H electric resistance welded tubing.

Outside Diameter (mm) Available Wall Thickness Range (mm)
21 1.5–4.0
25
27
32
38
42
48
51
57
60
63.5
76

Note: These are reference outside diameters within the stated manufacturing range. The availability of each OD and WT combination should be confirmed before ordering.

 

Corrosion Resistance of SPA-H Weathering Steel Pipe

SPA-H is an atmospheric corrosion-resistant steel. When exposed to suitable outdoor conditions, its surface gradually develops a rust-colored layer containing corrosion products. A stable and adherent weathering layer can reduce further corrosion of the steel substrate.

 

SPA-H steel contains copper, chromium, nickel and phosphorus within specified limits. These elements contribute to the corrosion behavior of the steel during atmospheric exposure.

 

Applications of JIS G3125 SPA-H ERW Steel Pipe

SPA-H ERW Pipe for Container Manufacturing

SPA-H steel is used in container manufacturing because of its atmospheric corrosion resistance and mechanical properties. SPA-H ERW round steel tube can be considered for tubular components, support members and structural parts in container-related equipment, subject to the container design and material requirements.

 

SPA-H Weathering Steel Pipe for Railway and Transportation

SPA-H welded steel tubing can be used in railway and transportation structures where weathering steel is specified. Typical components may include structural supports, equipment frames, protective structures and other fabricated tubular members.

 

SPA-H ERW Steel Tube for Structural Applications

SPA-H electric resistance welded tubing can be used in outdoor steel structures, support frames, architectural structures and fabricated components. The required pipe dimensions, load-bearing capacity, weld design and corrosion allowance should be determined by the project engineer.

 

SPA-H Welded Pipe for Industrial Equipment

SPA-H ERW steel pipes can be used in industrial equipment frames, machinery supports and outdoor installations requiring atmospheric corrosion-resistant steel. For fluid conveyance or pressure service, the applicable pressure-piping standard and design requirements must be confirmed separately.

SPA-H electric resistance welded pipes
spa-h erw steel tubes
SPA-H ERW Corten Steel Tubes

SPA-H ERW Steel Pipe Quality Control

GNEE can arrange inspection according to the agreed purchase specification and manufacturing requirements.

Inspection Item
Material Verification
MTC Review
Outside Diameter
Wall Thickness
Pipe Length
Straightness
Weld Seam
Surface Condition
NDT
Hydrostatic Test
Marking

The inspection method and acceptance criteria should be defined in the order. NDT methods may include ultrasonic testing or other suitable methods when specified. Hydrostatic testing should only be applied where required by the agreed product specification or service conditions.

SPA-H ERW Corten Steel Tubes
SPA-H erw round steel pipe
spa-h erw welded steel pipes

SPA-H ERW Steel Pipe Packaging and Delivery

SPA-H electric resistance welded pipes are packed according to pipe dimensions, surface condition and transportation requirements. Packaging may include:

  • Bundling with steel straps
  • Protective wrapping
  • End protection where required
  • Pipe identification labels
  • Heat number and batch traceability
  • Wooden supports or export packing where agreed

Delivery time depends on stock availability, raw material procurement, pipe dimensions, order quantity, production schedule and inspection requirements. The confirmed lead time will be provided with the quotation.

SPA-H erw welded steel pipes
SPA-H erw welded steel pipes
SPA-H Corten Steel Pipe

Request A Quote For JIS G3125 SPA-H Electric Resistance Welded Pipe

 

GNEE supplies JIS G3125 SPA-H electric resistance welded pipe, SPA-H ERW steel tube, and SPA-H straight seam welded pipe for industrial and structural applications.

 

Contact GNEE to request an SPA-H ERW steel pipe quotation, available sizes, technical specifications, and material certification.