ASTM A847 Corten Steel Welded Pipes

Nov 24, 2026 Leave a message

What Is ASTM A847 Corten Steel?

ASTM A847/A847M is a specification covering cold-formed welded and seamless high-strength low-alloy (HSLA) structural tubing with improved atmospheric corrosion resistance.

 

It applies to round, square, rectangular and special-shaped steel tubing used in welded, riveted or bolted structural construction, including bridges, buildings and general engineering applications.

 

Unlike conventional carbon steel tubing, ASTM A847 Corten Steel Welded Pipes contain controlled alloying elements, including copper, chromium, nickel and silicon.

 

These elements contribute to the development of a protective oxide layer when the material is exposed to suitable atmospheric conditions. This reduces the rate of atmospheric corrosion compared with conventional carbon steel in many environments.

 

Gnee supplies ASTM A847 weathering steel welded pipes for structural engineering, bridge construction, outdoor architectural structures and infrastructure projects.

 

Available configurations include round steel pipes, square steel tubes and rectangular steel tubes. Products can be manufactured according to specified outside dimensions, wall thicknesses, lengths and end preparations.

 

ASTM A847 specifies a minimum yield strength of 50,000 psi (345 MPa) and a minimum tensile strength of 70,000 psi (485 MPa). For tubing with a specified wall thickness of 0.120 in (3.0 mm) or greater, the minimum elongation is 19%.

ASTM A847 Corten Steel
ASTM A847 weathering steel welded pipes

These properties make ASTM A847 high-strength low-alloy steel tubing suitable for structural members requiring both load-bearing capacity and atmospheric corrosion resistance.

 

ASTM A847 Corten Steel Welded Pipes Specifications

Item Specification
Product Name ASTM A847 Corten Steel Welded Pipes
Manufacturing Process Cold Forming + Electric Resistance Welding (ERW) or Electric Fusion Welding (EFW)
Minimum Yield Strength 50,000 psi / 345 MPa
Minimum Tensile Strength 70,000 psi / 485 MPa
Minimum Elongation 19% (Wall Thickness ≥ 3.0 mm)
Wall Thickness 3.2–15.9 mm (Indicative Supply Range)
Square Tubes 3 in–12 in (Indicative Supply Range)
Rectangular Tubes 4 in × 2 in–16 in × 8 in (Indicative Supply Range)

 

ASTM A847 Corten Steel Pipe Chemical Composition

 

Chemical Requirements of ASTM A847 Steel

Element Heat Analysis (%) Product Analysis (%)
Carbon (C) 0.20 max 0.24 max
Manganese (Mn) 1.35 max 1.40 max
Phosphorus (P) 0.04 max 0.04 max
Sulfur (S) 0.035 max 0.045 max
Copper (Cu) 0.20 min 0.18 min
Nickel (Ni) Report Report
Chromium (Cr) Report Report
Silicon (Si) Report Report

 

Mechanical Properties of ASTM A847 Weathering Steel Tubes

ASTM A847 establishes minimum tensile properties for round and shaped structural tubing. 

Mechanical Property Requirement
Minimum Yield Strength 50,000 psi / 345 MPa
Minimum Tensile Strength 70,000 psi / 485 MPa
Minimum Elongation in 2 in (50 mm) 19%
Elongation Applicable Wall Thickness ≥ 0.120 in / 3.0 mm

For wall thicknesses below 0.120 in (3.0 mm), elongation requirements shall be agreed upon between the purchaser and manufacturer.

 

The minimum yield strength of 345 MPa provides the specified resistance to permanent deformation under tensile loading. The minimum tensile strength of 485 MPa defines the minimum maximum stress sustained before tensile failure. 

 

ASTM A847 Welded Steel Pipe Manufacturing Process

ASTM A847 welded structural tubing is manufactured from flat-rolled high-strength low-alloy steel. The manufacturing process includes material preparation, cold forming, longitudinal welding, sizing, cutting and inspection.

 

1. Raw Material Preparation

Flat-rolled weathering steel is selected according to the required ASTM A847 chemical composition and mechanical properties. The steel coil or plate is inspected for thickness, surface condition and material identification before forming.

 

2. Cold Forming

The steel strip is passed through forming rolls to produce the required round, square or rectangular cross-section. During cold forming, the strip edges are brought together to prepare the longitudinal joint.

 

3. Longitudinal Welding

ASTM A847 welded tubing is manufactured using electric resistance welding (ERW) or electric fusion welding (EFW). The longitudinal butt joint is welded through the wall thickness to ensure that the structural design strength of the tubing section is maintained.

 

No outside filler metal is added in the conventional ERW process. The weld seam position and finishing requirements can be specified according to the product shape and project requirements.

 

4. Sizing and Cutting

After welding, the tubing passes through sizing equipment to achieve the specified outside dimensions and cross-sectional geometry. The finished tubes are cut to random or fixed lengths according to the purchase order.

 

5. Inspection and Testing

Finished ASTM A847 Corten Steel Welded Pipes undergo dimensional inspection, surface examination and specified mechanical and chemical testing. Inspection records are prepared for order verification and material traceability.

ASTM A847 Corten Steel Welded Pipes
ASTM A847 Steel Tubing
ASTM A847 Welded Pipes

ASTM A847 Steel Tubing Dimensions and Tolerances

ASTM A847 covers round, square, rectangular and special-shaped structural tubing. Dimensional requirements depend on the cross-sectional shape, specified outside dimensions, wall thickness and ordered length.

 

The following table provides indicative product dimensions based on the available manufacturing range.

Product Shape Indicative Size Range
Round Weathering Steel Pipe 6.625 in, 8.625 in, 10.75 in, 12.75 in, 14 in, 16 in OD
Square Corten Steel Tube 3 in–12 in
Rectangular Corten Steel Tube 4 in × 2 in–16 in × 8 in
Wall Thickness 0.125 in–0.625 in
Length Single Random, Double Random, Fixed Length

 

ASTM A847 Dimensional Tolerances

For square and rectangular tubing, ASTM A847/A847M-21 specifies the following outside-dimension tolerances:

Largest Outside Dimension Across Flats Permissible Variation
2.5 in (63.5 mm) and under ±0.020 in (±0.5 mm)
Over 2.5 in to 3.5 in (88.9 mm), inclusive ±0.025 in (±0.6 mm)
Over 3.5 in to 5.5 in (139.7 mm), inclusive ±0.030 in (±0.7 mm)
Over 5.5 in (139.7 mm) ±1%

The specified minimum wall thickness at any measurement point shall not be more than 10% below the specified wall thickness. The maximum wall thickness, excluding the weld seam, shall not exceed the specified wall thickness by more than 10%.

 

For rectangular sections, the outside-dimension tolerance is calculated based on the larger flat dimension. Additional tolerance provisions may apply to the smaller dimension depending on the ratio between the external sides.

 

ASTM A847 Corten Steel Welded Pipes vs ASTM A500 Steel Tubes

ASTM A847 and ASTM A500 both cover structural steel tubing, but they address different material requirements.

 

ASTM A500 covers cold-formed welded and seamless carbon steel structural tubing, while ASTM A847 covers high-strength low-alloy structural tubing with improved atmospheric corrosion resistance.

Comparison ASTM A847 ASTM A500 Grade B
Material Type HSLA Weathering Steel Carbon Steel
Manufacturing Cold-Formed Welded and Seamless Cold-Formed Welded and Seamless
Minimum Yield Strength 345 MPa 290 MPa (Round)
Minimum Tensile Strength 485 MPa 400 MPa (Round)
Atmospheric Corrosion Resistance Improved No equivalent weathering requirement
Typical Applications Bridges, Outdoor Structures, Exposed Architectural Steel Building Frames, General Structural Tubing

 

Typical Applications of ASTM A847 Weathering Steel Pipes

ASTM A847 Corten Steel Welded Pipes are used in structural projects where the combination of mechanical strength, tubular geometry and atmospheric corrosion resistance is required.

1. Bridge Construction

Round, square and rectangular ASTM A847 structural tubes can be used in bridge components, exposed structural members, pedestrian bridge frameworks and supporting structures. Their specified minimum yield strength of 345 MPa supports structural design requirements, while their weathering characteristics make them suitable for properly detailed exposed steel structures.

 

2. Highway Signposts and Sign Structures

ASTM A847 weathering steel tubes are used in highway sign supports, sign frames and roadside structures. Square and rectangular tubing can be fabricated into structural support members for outdoor installations.

 

3. Architectural Exposed Steel Structures

ASTM A847 Corten Steel Welded Pipes are used in outdoor pavilions, architectural frames, landscape structures and exposed steel building components. The natural weathering surface can be incorporated into architectural designs without conventional painting where the exposure conditions are suitable.

 

4. Fencing and Outdoor Infrastructure

Weathering steel square tubes and rectangular tubes are used in fence posts, perimeter structures, outdoor barriers and infrastructure support frames. Their material composition is intended to improve resistance to atmospheric corrosion compared with conventional carbon steel.

 

5. Industrial Structural Applications

ASTM A847 structural tubing can be incorporated into equipment support frames, industrial platforms, outdoor pipe supports and other structural assemblies where the specified mechanical properties and atmospheric exposure conditions are appropriate.

 

ASTM A847 Testing and Inspection

Gnee can arrange inspection and testing according to the applicable ASTM A847 requirements and the agreed purchase order.

  • Chemical Analysis: Heat analysis and product analysis, where required, are used to verify the specified chemical composition.
  • Tensile Testing: Tensile tests are performed to verify the minimum yield strength, tensile strength and applicable elongation requirements.
  • Dimensional Inspection: Outside dimensions, wall thickness, length, straightness and cross-sectional geometry are checked against the order specifications.
  • Visual Inspection: Surface condition, forming defects, weld appearance and end preparation are examined.
  • Weld Inspection: The longitudinal weld is inspected according to the applicable manufacturing and project requirements. Additional nondestructive testing can be specified when required by the purchaser.
  • Material Traceability: Heat numbers and inspection records are maintained to support material identification and MTC documentation.

 

 

Lead Times and Packaging

Gnee supplies ASTM A847 Corten Steel Welded Pipes for project-based procurement, including trial orders and bulk structural steel requirements.

 

Products can be supplied in single random lengths, double random lengths or fixed lengths according to the purchase order. Plain ends and beveled ends are available according to fabrication and installation requirements.

 

For export transportation, the pipes can be bundled with steel straps and protected with suitable wrapping or wooden packaging according to product dimensions and shipping requirements. End protection can be arranged to reduce damage during handling and transportation.

 

 

The delivery schedule depends on the required dimensions, wall thickness, production quantity, testing requirements and stock availability. A production and delivery schedule will be confirmed after technical specifications and order quantities are reviewed.

A847 Structural Steel Tube
A847 electric resistance welded pipe
A847 ERW steel pipe

Request A Quote For ASTM A847 Corten Steel Welded Pipes

 

Are you looking for ASTM A847 Corten Steel Welded Pipes for bridge construction, highway infrastructure, outdoor architectural structures or industrial engineering projects?

 

Gnee supplies ASTM A847 weathering steel welded pipes in round, square and rectangular configurations. We can review your drawings and technical requirements to confirm the available dimensions, wall thickness, production process, testing scope and delivery schedule.

 

Contact Gnee today to request an ASTM A847 Corten Steel Welded Pipes quotation and technical specifications for your project.