JIS G3114 SMA 50 AW structural weathering steel plate

Sep 04, 2025 Leave a message

SMA 50 AW Steel Description

 

SMA 50 AW steel is a structural weathering steel which is also referred to as atmospheric corrosion resistant steel. SMA 50 AW steel chemical composition can increase resistance to atmospheric corrosion compared to other steels.

 

SMA 50 AW Steel

 

This is because it forms a protective layer on SMA 50 AW steel surface under the influence of the weather, So which could more accurately be termed as an "Atmospheric Corrosion Resistant Steel".

 

SMA 50 AW steel Delivery condition

 

Hot Rolled, Cold Rolled, Normalized, Quenched, Tempering, Thermal Mechanical Control Process (TMCP), Electroslag Remelting Technical, HIC test.

 

SMA 50 AW steel application

 

Due to the super property, SMA 50 AW steel has a widely use in Mine fans, earth moving buckets, trailers and large road vehicles, drill rings, cranes, excavators, underground mining equipment, bridges and other high strength components requiring superior toughness.

SMA 50 AW Steel Application

SMA 50 AW steel chemical composition by [%]

 

C Si Mn P S Cr N Cu CEV

Max 0.16

Max 0.5

0.5 - 1.5

Max 0.035

Max 0.035

0.4 -0.8

Max 0.009

0.25-0.55

Max 0.52

*Note:
1. The steels may show a Ni content of max 0.65 %;


2. For long SMA 50 AW steel, the P and S content can be 0.005% higher;


3. The SMA 50 AW steel may contain max. 0.30 % Mo and max. 0.15 % Zr


4. It is permissible to exceed the specified values provided that for each increase of 0.001 % N, the P max. content will be reduced by 0.005 %; the N content of the ladle analysis, however, shall not be more than 0.012 %


5.The max. value for nitrogen does not apply if the chemical composition shows a minimum total Al content of 0.020 % or if sufficient other N binding elements are present.

 

 

 

 

 

 

 

 

 

SMA 50 AW steel Mechanical properties

 

Nominal thickness (mm) to 16 16-40 40-63 63-80 80-100 100-150
ReH - Minimum yield strength (MPa) 355 345 335 325 315 295
Nominal thickness (mm) To 3 3-100 100-150
Rm -Tensile strength (MPa) 510-680 470-630 450-600
Nominal thickness (mm) 3-40 40-63 63-100 100-150
A - Minimum elongation Lo = 5,65 √ So (%) 22 21 20 18
Nominal thickness (mm) 1.5 - 2 2-2.5 2.5-3
A - Minimum elongation Lo = Lo = 80 mm (%) 16 17 18
Temperature -20 0
Notch impact test. Min. absorbed energy 27

27

 

 

 

 

 

 

 

 

 

 

 

 

 

Contact now to get SMA 50 AW Quote

About Us

 

Gnee operates a state-of-the-art manufacturing plant covering over 20,000 square meters, equipped with cutting-edge machinery and streamlined production lines. We focus on both efficiency and precision, ensuring top-quality output at every stage.

 

Our Key Equipment Includes:

 

 CNC plasma & laser cutting machines

 

 Large-scale bending, stamping, and integrated welding systems

 

 Fully automated sandblasting and coating lines

 

 In-house testing labs for strength and corrosion resistance

 

 Spacious, professional office spaces

 

From custom design to fabrication and final delivery, every step is handled in-house, giving us full control over quality, timing, and cost.

 

At Gnee, we integrate modern plant management and smart manufacturing to deliver efficient and reliable steel solutions worldwide.

JIS G3114 SMA 50 AW