What About the Hot rolled anti corrosion SPA-H steel plate

Jan 06, 2026 Leave a message

SPA-H steel plateAnti-corrosion SPA-H steel plate is produced by a hot-rolling process in accordance with JIS G3125, while SPA-C is supplied in cold-rolled condition.

 

Hot-rolled SPA-H is also known as SPA-H weathering steel plate or atmospheric corrosion-resistant steel plate. As the name indicates, SPA-H steel offers excellent resistance to atmospheric corrosion, making it an ideal material for long-term outdoor applications without the need for frequent painting or maintenance.

 

SPA-H weathering steel develops a stable, protective rust patina when exposed to the atmosphere, which significantly slows further corrosion.

 

Compared with ordinary carbon steel, SPA-H provides a much longer service life and lower life-cycle costs, especially in harsh outdoor environments such as bridges, buildings, containers, and structural components.

 

Gnee Steel not only supplies freshly produced SPA-H steel plates, but also maintains regular stock to meet urgent delivery requirements.

 

Hot Rolled SPA-H Anti-Corrosion Steel Plate Stock

 

Description Specification Price (USD/MT)
Weathering resistant steel plate SPA-H 3 × 1500 × C 768.66
Weather resistant steel plate SPA-H 5 × 1500 × C 768.66
SPA-H weathering steel plate 5 × 1500 × C 768.66
High tensile SPA-H weather corrosion steel plate 5 × 1500 × C 768.66
Hot rolled anti-corrosion SPA-H steel plate 8 × 1500 × C 768.66
Weather resistant steel plate SPA-H 2 × 1173 × C 768.66
Atmospheric corrosion resisting SPA-H steel plate 8 × 1500 × C 768.66
New material SPA-H steel plate 3 × 1500 × C 768.66
SPA-H corten steel plate 2.9 × 1125 × C 768.66
SPA-H corrosion resistant steel plate 5 × 1110 × C 768.66
SPA-H weathering resistant steel 3 × 1500 × C 768.66
SPA-H high strength low alloy steel plate 10 × 1500 × C 768.66

 

For standard hot-rolled SPA-H steel plates, Gnee Steel usually has sufficient stock and can arrange delivery within 10 days.


For special sizes that cannot be obtained through further processing of standard plates, we can arrange customized production according to your project requirements.

 

Contact now

 

info-621-645

 

What is spa H material?

As Spa-h steel coil material is a weathering steel, it forms the protective patina on the surface which gives it a rustic appearance. The chemical composition of the JIS g3125 spa-h strip includes carbon, silicon, manganese, phosphorus, sulphur, copper, chromium and nickel.

 

What is spa-h steel equivalent?

Worldwide equivalents of grade SPA-H (Japan: JIS ) Cross reference table for Steel SPA-H (JIS ) and its European equivalent S355J0WP (1.8945)

 

What is the chemical composition of SPA-H Steel?

The main elements include carbon (C), manganese (Mn), silicon (Si), chromium (Cr), and copper (Cu). Their contents are strictly controlled to ensure mechanical properties and weather resistance.

 

How to maintain SPA-H Steel?

SPA-H steel requires minimal maintenance. A stable rust layer protects the steel. Regular cleaning to remove dust or debris and avoiding prolonged water exposure is sufficient.

 

Can SPA-H Steel be welded?

Yes. Low-hydrogen arc welding or gas shielded welding is recommended. Preheating and slow cooling after welding help prevent cracking.

 

CORTEN Corten A Corten B    
ASTM A588/A588M A588 Grade A A588 Grade B A588 Grade C A588 Grade K
ASME SA588/SA588M SA588 Grade A SA588 Grade B SA588 Grade C SA588 Grade K
EN 10025-5 S235J0W S235J2W S355J0WP S355J2WP
S355J0W S355J2W S355K2W  
EN 10155 S235J0W S235J2W    
S355J0WP S355J2WP    
S355J0W S355J2G1W S355J2G2W S355K2G1W
S355K2G2W      
TB/T 1979 08CuPVRE 09CuPTiRE-A 09CuPTiRE-B 09CuPCrNi-A
09CuPCrNi-B 05CuPCrNi    
GB/T 4171 Q295GNH Q345GNH Q265GNH Q310GNH
Q235NH Q295NH Q355NH Q415NH
Q460NH Q500NH Q550NH  
JIS G 3114 SMA400AW SMA400BW SMA400CW  
SMA400AP SMA400BP SMA400CP  
SMA490AW SMA490BW SMA490CW  
SMA490AP SMA490BP SMA490CP  
SMA570W SMA570P    
JIS G3125 SPA-H SPA-C