What are the grades of ASME SA588 grade C weathering steel plate

Nov 18, 2025 Leave a message

Product Overview
SA588 Grade C weathering steel plate is a high-strength, low-alloy structural steel specified under ASME SA588 / SA588M standards. It is designed to resist atmospheric corrosion by forming a self-protecting rust-like patina, reducing the need for painting and long-term maintenance.

SA588 Grade C weathering steel plate

This steel plate is widely applied in bridge construction, shipping containers, tanks, vessels, railway carriages, and other structural engineering projects. Its combination of high strength, toughness, and corrosion resistance ensures reliability even in harsh outdoor environments.

 

Specifications

Property Value
Steel Grade SA588GrC
Standard ASME SA588 / SA588M
Thickness 4mm – 450mm
Width 1000mm – 4200mm
Length 3000mm – 18000mm
Production Method Hot Rolled
Delivery Condition Normalized (N), Quenched & Tempered (Q+T), TMCP (Thermal-Mechanical Control Process), or as required

 

Chemical Composition (wt%)

Element Max / Range
C (Carbon) 0.20
Mn (Manganese) 0.75 – 1.35
P (Phosphorus) 0.04
S (Sulfur) 0.05
Si (Silicon) 0.15 – 0.50
Ni (Nickel) 0.50
Cr (Chromium) 0.40 – 0.70
Cu (Copper) 0.20 – 0.40
V (Vanadium) 0.01 – 0.10

Controlled alloying provides excellent corrosion resistance, high strength, and good weldability without compromising toughness.

 

Mechanical Properties

Property SA588 Grade C Plate
Tensile Strength 400 – 650 MPa
Yield Strength ≥ 250 MPa
Elongation ≥ 20% (2 in / 50mm gauge)
Impact Test Temperature +20 °C, 0 °C, −20 °C

The steel plate meets high-strength and low-temperature toughness requirements, making it suitable for outdoor and load-bearing applications.

 

Surface Treatment Options

Shot blasting

Painting or coated

Customized finishes available

These treatments further enhance durability and aesthetics for structural or decorative applications.

 

Applications

Bridge Construction: Girders, beams, and supporting structures

Shipping Containers & Storage Tanks: Long-term atmospheric corrosion resistance

Vessels & Industrial Equipment: Durable and high-strength load-bearing applications

Railway Carriages & Machinery: Structural steel requiring toughness and durability

Other Construction Projects: Highway structures, frameworks, and outdoor installations

 

Why Choose Gnee Steel Plate?

Certified Quality: Manufactured according to ASME SA588 / SA588M standards

Competitive Price: Cost-effective solutions with large-scale production

Reliable Supply: 5,000 – 10,000 MT per month, depending on thickness and size

Technical Support: Guidance on specifications, welding, and application design

 

For SA588 Grade C weathering steel plate prices or technical consultation, contact Gnee Steel directly for expert assistance and fast quotations.

 