Products Description
S355J2W N STEEL PLATES are best recognized for their amazing alloy properties, mainly because the alloy helps plates to work successfully in any temperature conditions.
If the alloy selection is wrong, it can make the product useless. Thus, S355J2W+N alloy is ideal because of its excellent mechanical and chemical properties. Such plates are nonferrous plates are much in demand in engineering application usage as well.

S355J2W+N is structural steel which is also weather resistant. It is designed with a layer known as a barrier layer which is formed when the S355J2W N STEEL PLATES come in contact with the reducing environment conditions.
In addition, such plates also offer excellent resistance properties such as corrosion-resistant, pitting, and crevice-resistant; it is resistant to oxidation, chloride stress, cracking corrosion, etc.
Products Specification
| Item | Specification |
|---|---|
| Standard | EN 10025 |
| Width | 1000 mm – 4500 mm |
| Thickness | 5 mm – 150 mm |
| Length | 3000 mm – 18000 mm |
| Material Grades | S355J0W, S355J2W, S355J2W+N |
| Process | Hot Rolled (HR) |
S355J2W+N Plate Processing
1. Cutting
S355J2W+N Corten steel plates can be cut to required sizes using advanced methods such as plasma cutting, laser cutting, or flame cutting. Precise cutting ensures clean edges and accurate dimensions, making the plates ready for fabrication and assembly with minimal post-processing.
2. Forming
The material offers excellent formability and can be shaped through bending, rolling, or pressing to meet specific design requirements. Whether used for architectural panels or structural components, S355J2W+N steel maintains its strength and weathering properties after forming.
3. Drilling / Machining
S355J2W+N plates are easily drillable and machinable with conventional equipment. Holes, slots, and custom features can be added to meet exact construction or engineering needs without compromising mechanical performance or corrosion resistance.
4. Grinding
Surface grinding and finishing operations can be applied to achieve smooth, uniform textures or to prepare the steel for further surface treatment. This process enhances the aesthetic appeal, especially for architectural and decorative applications where surface quality is critical.
5. Testing
Every S355J2W+N Corten steel plate undergoes strict quality testing, including mechanical strength, chemical composition, ultrasonic, and impact resistance tests. These ensure that each plate meets international standards and delivers consistent performance in demanding environments.
Chemical Composition of S355J2W+N Plate
| C | Si | Mn | P | S | Cr | Zr | Ni | Cu | Mo | CEV |
| 0.16 max. | 0.50 max. | 0.50 max. | 0.03 max. | 0.03 max. | 0.40-0.80 | 0.15 max. | 0.65 max. | 0.25-0.55 | 0.03 max. | 0.44 max. |
Mechanical Properties of S355J2W+N Plate
| Yield Strength | Tensile Strength | Minimum Elongation A (Lo = 5.65 vSo) % |
| 355 MPa | 510 - 680 MPa | 20 |
Products Application