ASTM A423 Grade 1 corten boiler steel tube

Nov 23, 2026 Leave a message

What is the ASTM A423/A423M standard?

ASTM A423/A423M is an American material specification covering minimum-wall-thickness seamless and electric-resistance welded low-alloy steel tubes for pressure-containing components, particularly boiler economizers and other applications requiring corrosion resistance.

 

The standard covers three material grades: Grade 1, Grade 2 and Grade 3. It specifies chemical composition, tensile properties, heat treatment, manufacturing requirements and mechanical testing procedures.

 

ASTM A423 Grade 1 has a minimum tensile strength of 415 MPa, a minimum yield strength of 255 MPa and a minimum elongation of 25%. The commonly supplied outside diameter ranges from 21 to 76 mm, with minimum wall thicknesses from 1.5 to 4.0 mm.

 

What is ASTM A423 Grade 1 ERW Boiler Steel Tube?

ASTM A423 Grade 1 ERW boiler steel tube is a low-alloy steel tubular product manufactured through electric resistance welding (ERW). It is designed for pressure-containing components such as boiler economizers and industrial heat-transfer equipment where specified mechanical properties and corrosion resistance are required.

 

During ERW manufacturing, low-alloy steel strip is progressively formed into a tubular section. Electrical resistance generates heat at the adjoining edges, and mechanical pressure joins them to create a continuous longitudinal weld seam. The tube is subsequently subjected to the specified heat treatment, sizing, cutting and inspection procedures.

Product Characteristics

Material Standard: ASTM A423/A423M

Grade: Grade 1

Manufacturing Process: ERW (Electric Resistance Welding)

Material Classification: Low-Alloy Steel

Minimum Tensile Strength: 415 MPa

Minimum Yield Strength: 255 MPa

Minimum Elongation: 25%

Main Applications: Boiler Economizers and Pressure-Containing Components

ASTM A423 Grade 1 ERW boiler steel tube
A423 Grade 1 ERW Boiler Steel Tube

ASTM A423 Grade 1 Boiler Steel Tube Specifications & Standards

Parameter  Technical Specification
Product Name  ASTM A423 Grade 1 Boiler Steel Tube
Material Grade  ASTM A423 Grade 1 / A423 Gr.1
Governing Standard  ASTM A423/A423M
Related ASME Standard ASME SA-423, when specified
Material Classification  Low-Alloy Steel
Manufacturing Process ERW 
Manufacturing Finish  Hot Finished / Cold Finished 
Outside Diameter  21-76 mm (commonly furnished range)
Wall Thickness  1.5-4.0 mm (minimum wall thickness)
Tensile Strength ≥ 415 MPa
Yield Strength ≥ 255 MPa
Elongation ≥ 25%
Tube End Plain End / Beveled End 

 

Chemical Composition of ASTM A423 Grade 1 (wt.%)

ASTM A423 Grade 1 uses a controlled low-alloy chemical composition containing copper, chromium and nickel. These alloying elements contribute to the material's corrosion-resistant characteristics.

 

The chemical requirements are specified separately for each element, with maximum, minimum or range limits.

ASTM A423 Grade 1 

Element Chemical Composition
Carbon (C)  ≤ 0.15%
Manganese (Mn)  ≤ 0.55%
Phosphorus (P)  0.06–0.16%
Sulfur (S)  ≤ 0.060%
Silicon (Si)  ≥ 0.10%
Copper (Cu)  0.20–0.60%
Chromium (Cr)  0.24–1.31%
Nickel (Ni)  0.20–0.70%

 

Mechanical Properties of ASTM A423 Grade 1 Boiler Tubes

ASTM A423 Grade 1 boiler tubes must meet the tensile requirements specified by the standard. The minimum tensile strength is 60 ksi (415 MPa), and the minimum yield strength is 37 ksi (255 MPa).

 

The minimum elongation is 25% based on a 2-inch or 50 mm gauge length, subject to the applicable specimen requirements and elongation adjustments.

ASTM A423 Grade 1

Mechanical Property  Requirement
Tensile Strength  ≥ 415 MPa
Yield Strength ≥ 255 MPa
Elongation  ≥ 25%
Tensile Test Standard  ASTM A370
Gauge Length 50 mm / 2 in.
Brinell Hardness  ≤ 170 HBW
Rockwell Hardness  ≤ 87 HRBW

 

Mechanical Performance Analysis

The minimum yield strength of 255 MPa defines the stress level at which permanent deformation begins under the specified tensile test conditions. The minimum tensile strength of 415 MPa specifies the required maximum tensile stress before failure. The minimum elongation of 25% indicates the required tensile deformation capacity.

 

For boiler and heat-transfer equipment, these properties are important when selecting steel tubes subjected to internal pressure, thermal expansion, bending and installation loads. 

 

ASTM A423 Grade 1 Boiler Tube Manufacturing Process

ASTM A423 Grade 1 ERW boiler steel tubes are manufactured through a controlled production process involving steel strip preparation, roll forming, electric resistance welding, heat treatment, sizing, cutting and inspection.

 

During production, steel strip is first inspected for surface quality and chemical composition. The strip then passes through a series of forming rolls to create a tubular shape. High-frequency electrical resistance heating is applied to the adjoining edges, followed by pressure welding to produce a continuous longitudinal seam.

 

After welding, the tube undergoes the required heat treatment and sizing operations. The finished tubes are cut to the specified length and subjected to dimensional, mechanical and other applicable inspection procedures.

A423 Grade 1 Boiler Steel Tube
ASTM A423 Grade 1 ERW boiler steel tubes
ASTM A423 Grade 1 Boiler Tube

Manufacturing Process Table 

Manufacturing Stage 
1. Raw Material Inspection 
2. Strip Preparation 
3. Roll Forming 
4. ERW Welding 
5. Heat Treatment 
6. Sizing and Straightening 
7. Cutting
8. Final Inspection 

ERW Weld Seam Quality Control

For ASTM A423 Grade 1 ERW boiler tubes, the longitudinal weld seam is an important manufacturing control point. Welding temperature, edge alignment, welding pressure and production speed must be controlled during the welding process.

 

The finished tube is inspected according to the applicable ASTM A423/A423M requirements and purchase specification. Hydrostatic testing or an applicable electric test is performed according to the specified inspection option.

 

ASTM A423 Grade 1 Boiler Tube Heat Treatment

Heat treatment is an important part of ASTM A423 Grade 1 boiler tube manufacturing. The standard requires tubes to be normalized or subjected to the heat treatment necessary to meet its specified requirements.

 

For ERW boiler tubes, heat treatment is controlled according to the manufacturing process and applicable standard requirements. Normalizing involves heating the steel to an appropriate temperature above its transformation range, holding it for the required period and cooling it in still air.

 

This process is used to establish the required metallurgical condition and mechanical properties of the finished tube.

 

Heat Treatment Item
Heat Treatment 
Heating
Holding
Cooling
Final Verification 

 

 

Applications of ASTM A423 Grade 1 Boiler Steel Tubes

ASTM A423 Grade 1 steel tubes are primarily used in boiler and industrial heat-transfer systems where pressure containment and corrosion resistance are required. Their specified mechanical properties and low-alloy composition make them suitable for economizers and other applications covered by ASTM A423/A423M.

 

1. Boiler Economizer Tubes 

Boiler economizers recover heat from flue gas to preheat boiler feedwater before it enters the steam-generating system. ASTM A423 Grade 1 tubes can be used in economizer assemblies designed according to the applicable pressure and temperature requirements.

 

2. Heat Exchanger Tubes 

ASTM A423 Grade 1 tubes can be used in industrial heat-transfer equipment where the material specification and operating conditions are compatible. Tube selection depends on working pressure, temperature, fluid characteristics and corrosion conditions.

 

3. Boiler Pressure-Containing Components 

The ASTM A423 specification covers low-alloy steel tubes intended for pressure-containing components. Grade 1 tubes can be specified for applicable boiler components when their material properties, dimensions and design conditions meet the relevant requirements.

 

4. Industrial Heat Recovery Systems 

Industrial heat recovery equipment uses heat exchanger assemblies to transfer energy from exhaust gases or process fluids. ASTM A423 Grade 1 tubes may be used in compatible tubular components according to the specified operating conditions.

 

5. Industrial Heat-Transfer Equipment

These tubes can be specified for industrial equipment requiring tubular heat-transfer components with controlled chemical composition and mechanical properties.

A423 Grade 1 Boiler Tube
STM A423 Grade 1 boiler steel tubes
A423 Grade 1 boiler tubes

ASTM A423 Grade 1 Boiler Tube Quality Control & Inspection

Quality control for ASTM A423 Grade 1 boiler steel tubes includes chemical composition analysis, tensile testing, flattening testing, flaring testing, flange testing, reverse flattening testing, hardness testing and hydrostatic or electric testing as required by the applicable standard.

 

For ERW products, additional attention is given to longitudinal weld integrity, dimensional accuracy and surface condition. Inspection requirements are determined according to ASTM A423/A423M and the purchase order.

 

Test / Inspection Item
Chemical Analysis 
Tensile Test
Flattening Test 
Flaring Test
Flange Test 
Reverse Flattening Test
Hardness Test 
Hydrostatic Test 
Electric Test

 

 

ASTM A423 Boiler Steel Tube Dimensional Tolerances

Dimensional accuracy is important for ASTM A423 Grade 1 boiler tubes because outside diameter, minimum wall thickness and tube length affect installation, tube expansion and heat exchanger assembly.

 

ASTM A423 refers to the applicable general requirements for dimensional tolerances and inspection. The actual tolerances must be checked against the specified standard edition and ordered dimensions.

 

Dimensional Parameter Requirement 
Outside Diameter  12.7–127 mm commonly furnished 
Minimum Wall Thickness 0.9–12.7 mm commonly furnished 
Length Random or specified length 
Ovality According to applicable dimensional tolerance requirements
Straightness According to applicable dimensional tolerance requirements 
End Preparation Plain End / Other agreed preparation

 

Lead Time and Packaging

ASTM A423 Grade 1 boiler steel tubes can be supplied in bundles, wooden cases or other packaging configurations according to tube dimensions, wall thickness and shipping requirements. Proper packaging helps prevent surface damage, deformation and contamination during handling and transportation.

A423 Grade 1 boiler steel tubes
ASTM A423 Grade 1 ERW  Boiler Tube

Standard production lead time depends on raw material availability, tube dimensions, order quantity and heat treatment requirements. Each shipment can be supplied with the agreed quality documents and identification markings.

 

Item Supply Details
Production Lead Time  Confirmed according to order quantity and specifications 
Standard Length Random Length / Cut Length
Packaging  Steel Bundles / Wooden Cases 
Surface Protection  Anti-Rust Protection as Agreed 
End Protection  Plastic Caps if Required 
Shipping Mark  ASTM Standard, Grade, Size, Heat Number 
Quality Documents  Mill Test Certificate (MTC
Inspection Records  Chemical and Mechanical Test Reports 

 

Contact Gnee For ASTM A423 Grade 1 Boiler Steel Tube Supply

 

Gnee supplies ASTM A423 Grade 1 boiler steel tubes for industrial boiler systems, economizers and heat-transfer equipment. Our supply options include ERW and seamless low-alloy steel tubes, with specifications based on ASTM A423/A423M and customer requirements.

 

We can provide customized outside diameters, wall thicknesses and cutting lengths according to project specifications. Material documentation, chemical composition reports and mechanical test results can also be arranged according to the purchase agreement.

 

Whether you are sourcing ERW boiler tubes for economizer manufacturing or low-alloy steel tubes for industrial heat-transfer equipment, Gnee can assist with technical specifications, product selection and quotation arrangements.