Products Description
S235J0W is a low-alloy, weather-resistant structural steel grade under the EN 10025-5 standard. It is specifically designed to offer enhanced resistance to atmospheric corrosion compared with conventional carbon steels.
By adding alloying elements such as copper, chromium, and nickel, S235J0W forms a protective oxide layer - often called a patina - that prevents further rusting and extends the steel's service life.

With a minimum yield strength of 235 MPa and excellent weldability and formability, S235J0W is widely used in bridges, building façades, outdoor sculptures, and transportation structures where both durability and an attractive weathered appearance are desired.
Products Specification
|
Gnee Grade : |
S235J0W |
|
Specification: |
Thickness 8mm-300mm, Width: 1500-4020mm, Length: 3000-27000mm |
|
Standard: |
EN10025-5 Technical delivery conditions for general structural steels |
|
Approval By Third Party |
ABS, DNV, GL, CCS, LR , RINA, KR, TUV, CE |
|
Classification: |
hot rolled or normalizing structural steels |
Chemical composition
|
C |
Si |
Mn |
Cu |
P |
S |
Cr |
N |
|
0.16 |
0.45 |
0.15-0.70 |
0.20-0.60 |
0.040 |
0.040 |
0.35-0.85 |
0.010 |
Mechanical properties
|
Temperature |
-20 |
-10 |
0 |
20 |
|
Notch impact test. Min. absorbed energy J |
27 |
|
Nominal thickness (mm) |
to 16 |
16 - 40 |
40 - 63 |
63 - 80 |
80 - 100 |
100 - 150 |
|
ReH - Minimum yield strength (MPa) |
235 |
225 |
215 |
215 |
215 |
195 |
|
Nominal thickness (mm) |
to 3 |
3 - 100 |
100-150 |
|
Rm -Tensile strength (MPa) |
360-510 |
360-510 |
350-500 |
|
Nominal thickness (mm) |
≥1.5<2 |
≥2﹤2.5 |
≥2.5<3 |
≥3<40 |
≥40﹤63 |
≥6﹤100 |
≥100﹤150 |
|
A - Minimum elongation Lo = 5,65 √ So (%) Longitudinal |
19 |
20 |
21 |
26 |
25 |
24 |
22 |
Equivalent grades of grade S235J0W
|
UNI EU 155 |
France NFA35502 |
Germany WBL 087 |
U.K. BS 4360 |
Canada CSA G4021 |
USA ASTM |
|
Fe360 CK1 |
E 24W3 |
WSt 37-2 |
In conclusion, S235J0W weathering steel combines strength, durability, and aesthetic appeal in one versatile material. Its self-protecting rust layer not only enhances corrosion resistance but also eliminates the need for regular painting or maintenance, offering long-term cost savings.
With its excellent mechanical properties and natural weathered look, S235J0W is an ideal choice for architectural projects, outdoor structures, and environmentally sustainable designs that require both performance and visual impact.
Contact now to get S235J0W Quote