Products Description
The material number of S235J0W steel is 1.8958. S235J0W steel under EN 10025-5 standard is a kind of structural steel with improved atmospheric corrosion resistance steel. It is also called weathering steel or atmosphere corrosion resistance steel.

This EN 10025-5 European Standard specifies requirements for flat and long products of hot rolled steels with improved atmospheric corrosion resistance in the grades and qualities given in chemical composition tables and mechanical properties tables in the usual delivery conditions.
S235J0W Steel with Improved Atmospheric Corrosion Resistance
S235J0W steel has a minimum impact energy value of 27 J at 0℃.
Size range for S235J0W steel plate and flat bar is : 1.2-150mm * 1000-3800mm * 3000-18000 mm
Specification of S235J0W Steel
| Standard | EN 10025-5 |
| Grade | S235J0W, S235J0W+N |
| Category | Atmospheric resistant steel, weathering steel |
| Thickness | 1.2-150mm |
| Width | 1220-4200mm |
| Length | 5000-18000mm, or cut shapes as required |
| Form | Plates, sheets,coils, Plain Sheet, flat steel, section steel, H beams, bars, Perforated Sheet, Chequered Plate |
| Finish | Hot rolled plate (HR), Cold rolled sheet (CR) |
| Hardness | Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
| Grade | Corten Steel EN 10025 S235J0W+N |
Chemical Composition and Mechanical Property
| Grade | C MAX | Mn≥ | Si MAX | P MAX | S MAX | Cr | Cu |
| EN10155 S235J0W | 0.13 | 0.20-0.60 | 0.4 | 0.04 | 0.04 | 0.40-0.80 | 0.25-0.55 |
| Grade | Tensile Strength(MPa) | Yield Strength(MPa) | % Elongation in 2 in.(50mm) min | Impacting Test Temperature(°C) |
| EN10155 S235J0W | 360-510 | 235 | 24 | 0 |
Products Application
EN10155 S235J0W weather-resistant steel plate is widely used across various industrial and structural applications that require both strength and superior atmospheric corrosion resistance. Its unique composition allows it to form a stable, protective oxide layer when exposed to the atmosphere, significantly extending its service life even in harsh outdoor environments.
In addition to architectural and structural uses, S235J0W steel plate can also be applied in pressure-bearing and thermal equipment. As EN10155 S235J0W Pressure Vessel and Boiler Steel Plate, it is used in the manufacturing of pressure vessels, boilers, storage tanks, and heat exchangers within the oil, gas, chemical, and power generation industries. The material's excellent weldability and toughness ensure safe performance under high temperatures and varying pressure conditions.
Furthermore, its low maintenance requirements and aesthetic weathered finish make it a popular choice for bridge construction, container manufacturing, railway wagons, and industrial equipment housings.
With its combination of mechanical reliability and natural corrosion protection, EN10155 S235J0W steel plate offers a cost-effective and environmentally friendly solution for projects requiring long-term structural stability and visual appeal.
Contact now to get S235J0W Quote