Oct 16, 2025
This material is engineered with a precise chemical composition—containing approximately 0.06–0.12% Carbon, 0.25–0.75% Silicon, 0.50–1.25% Manganese,
Details
Oct 16, 2025
ND (09CrCuSb) steel tubes are widely used in the manufacture of economizers, air preheaters, heat exchangers and evaporators that are used in 100-high
Details
Oct 16, 2025
09CrCuSb Steel tubing is a low alloy structural steel.Compared with other types of steel such as mild steel, Corten, CR1A, ND steel has excellent corr
Details
Oct 14, 2025
Q460NH steel plate,under China GB/T 4171 standard, Q460NH steel plate is a kind of weathering steel. Q460NH steel plate is widely used to: container,
Details
Oct 14, 2025
China GB/T 4171 Q500NH Weather Resistant Steel plate,China GB/T 4171 Q500NH Weather Resistant Steel Plates,China GB/T 4171 Q500NH Weather Resistant St
Details
Oct 14, 2025
Q500NH steel plate major added metal elements are nickel, copper.GB/T 4171 Q500NH is one kind steel grade for atmosphere corrosion resistance.
Details
Oct 14, 2025
Q550NH Corten Steel Plate is another high-strength low-alloy (HSLA) steel, similar to other corten or weathering steel grades, but with a higher yield
Details
Oct 14, 2025
GB/T 4171 Q550NH steel plate can withstand long-term exposure to harsh weather, and is therefore also known as weathering steel or atmospheric corrosi
Details
Oct 14, 2025
Steel Standard:JIS G3114
Rolling Type:Corten steel,Weathering steel plate
Thickness:2mm-300mm
Width:1000mm-4200mm
Length:3000m
Details
Rolling Type:Corten steel,Weathering steel plate
Thickness:2mm-300mm
Width:1000mm-4200mm
Length:3000m
Oct 14, 2025
Steel Standard:JIS G3114
Rolling Type:Corten steel,Weathering steel plate
Thickness:2mm-300mm
Width:1000mm-4200mm
Length:3000m
Details
Rolling Type:Corten steel,Weathering steel plate
Thickness:2mm-300mm
Width:1000mm-4200mm
Length:3000m
Oct 14, 2025
SMA400CW corten steel conforms to the JIS G3114 standard and is widely used in air preheaters, economizers, railway carriages, container manufacturing
Details
Oct 14, 2025
Q310GNH, Q295NH, and Q355NH weathering steel plates are low-alloy high-strength steels (Weathering Steel) with excellent atmospheric corrosion resista
Details